Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.017 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.796 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCm [8] |
HallC 2y |
Point Groupm |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 0> | <1 0 -1> | 141.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 275.2 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 291.0 |
SiO2 (mp-6930) | <1 0 1> | <1 0 -1> | 141.4 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 291.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 174.6 |
ZnSe (mp-1190) | <1 1 0> | <1 0 -1> | 141.4 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 291.0 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 183.0 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 141.4 |
Te2W (mp-22693) | <1 0 0> | <0 1 0> | 291.0 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 135.4 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 291.0 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 91.7 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 291.0 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 183.5 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 291.0 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 291.0 |
BN (mp-984) | <1 1 0> | <1 0 0> | 275.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 1> | 183.0 |
BN (mp-984) | <0 0 1> | <0 1 0> | 174.6 |
BN (mp-984) | <1 0 0> | <1 0 0> | 275.2 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 275.2 |
MoS2 (mp-1434) | <1 0 1> | <1 0 0> | 275.2 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 275.2 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 291.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 291.0 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 174.6 |
SiC (mp-7631) | <1 0 1> | <0 1 1> | 147.4 |
TeO2 (mp-2125) | <0 0 1> | <1 1 1> | 192.0 |
SiC (mp-7631) | <1 0 0> | <0 1 0> | 291.0 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 291.0 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 1> | 192.0 |
GdScO3 (mp-5690) | <1 1 1> | <0 1 0> | 291.0 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 0> | 232.8 |
LaF3 (mp-905) | <0 0 1> | <1 0 1> | 183.0 |
LaF3 (mp-905) | <1 0 1> | <1 0 0> | 275.2 |
TbScO3 (mp-31119) | <0 1 0> | <0 1 0> | 174.6 |
TbScO3 (mp-31119) | <1 1 1> | <0 1 0> | 291.0 |
Ni (mp-23) | <1 1 1> | <0 1 0> | 291.0 |
PbSe (mp-2201) | <1 1 0> | <1 0 0> | 275.2 |
BaTiO3 (mp-5986) | <1 0 0> | <0 1 0> | 291.0 |
Ni (mp-23) | <1 0 0> | <0 1 0> | 174.6 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 275.2 |
NdGaO3 (mp-3196) | <1 1 1> | <1 0 0> | 275.2 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 291.0 |
CdSe (mp-2691) | <1 1 0> | <1 0 0> | 275.2 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 217.3 |
Au (mp-81) | <1 1 0> | <0 1 0> | 291.0 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 275.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TiP2O7 (mp-761041) | 0.3638 | 0.012 | 3 |
MnP2O7 (mp-770670) | 0.3555 | 0.246 | 3 |
TiP2O7 (mp-761010) | 0.3352 | 0.000 | 3 |
CoP2O7 (mp-31589) | 0.3551 | 0.061 | 3 |
CrP2O7 (mp-540291) | 0.3571 | 0.103 | 3 |
VFe(P2O7)2 (mp-767722) | 0.4071 | 0.009 | 4 |
VCr(P2O7)2 (mp-767779) | 0.4321 | 0.021 | 4 |
LiP5W3O19 (mp-763535) | 0.2059 | 0.099 | 4 |
LiV3P5O19 (mp-763368) | 0.1069 | 0.088 | 4 |
Ta2Cd(P2O7)3 (mp-559692) | 0.4340 | 0.000 | 4 |
Cr5O12 (mp-773920) | 0.6589 | 0.000 | 2 |
Nb2O5 (mp-776896) | 0.5735 | 0.059 | 2 |
V5O12 (mp-778252) | 0.6453 | 0.024 | 2 |
VCrP2(O4F)2 (mp-765139) | 0.5238 | 0.041 | 5 |
MgCr3Se2(SO6)4 (mp-769544) | 0.5394 | 0.126 | 5 |
MnVP2(O4F)2 (mp-777435) | 0.5450 | 0.002 | 5 |
MgCr3Se3(SO8)3 (mp-773999) | 0.5208 | 0.180 | 5 |
VFeP2(O4F)2 (mp-778349) | 0.5332 | 0.036 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Ti_pv P O |
Final Energy/Atom-7.7429 eV |
Corrected Energy-229.8552 eV
Uncorrected energy = -216.8022 eV
Composition-based energy adjustment (-0.687 eV/atom x 19.0 atoms) = -13.0530 eV
Corrected energy = -229.8552 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)