Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.244 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.95 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.661 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI41/a [88] |
HallI 4bw 1bw |
Point Group4/m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 192.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 251.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 125.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 125.6 |
TeO2 (mp-2125) | <0 0 1> | <1 0 1> | 192.0 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 1> | 192.0 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 125.6 |
Mg (mp-153) | <1 0 0> | <0 0 1> | 251.1 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 125.6 |
TbScO3 (mp-31119) | <0 0 1> | <0 0 1> | 125.6 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 1> | 192.0 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 145.2 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 125.6 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 1> | 192.0 |
WSe2 (mp-1821) | <0 0 1> | <1 0 1> | 192.0 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 125.6 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 251.1 |
NaCl (mp-22862) | <1 0 0> | <1 0 1> | 192.0 |
ZnO (mp-2133) | <1 1 1> | <0 0 1> | 125.6 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 251.1 |
SrTiO3 (mp-4651) | <1 1 0> | <0 0 1> | 125.6 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 251.1 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 125.6 |
ZnO (mp-2133) | <1 0 0> | <1 0 1> | 192.0 |
SrTiO3 (mp-4651) | <0 0 1> | <0 0 1> | 125.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiAgF2 (mp-753299) | 0.6100 | 0.095 | 3 |
Li2B2Se5 (mp-30100) | 0.5866 | 0.000 | 3 |
Na2Mn2O3 (mp-769934) | 0.5888 | 0.035 | 3 |
Ca3Al3N5 (mp-1029921) | 0.5737 | 0.000 | 3 |
Na3VO3 (mp-778022) | 0.5808 | 0.064 | 3 |
CsNa3TiO4 (mp-18182) | 0.4166 | 0.000 | 4 |
NaLi3SiO4 (mp-559904) | 0.2566 | 0.000 | 4 |
EuMg3SiN4 (mp-1019726) | 0.2796 | 0.530 | 4 |
CaMg3SiN4 (mp-1019579) | 0.2588 | 0.005 | 4 |
RbNa3SnO4 (mp-556968) | 0.2316 | 0.000 | 4 |
Sn3P4 (mp-684588) | 0.7418 | 0.211 | 2 |
In4Te3 (mp-617281) | 0.7285 | 0.000 | 2 |
In4Se3 (mp-19932) | 0.7368 | 0.027 | 2 |
Sr2AlGaCo2O7 (mvc-3397) | 0.7092 | 0.319 | 5 |
Sr2YGaW2O7 (mvc-359) | 0.6858 | 0.588 | 5 |
Sr2AlV2GaO7 (mvc-350) | 0.6766 | 0.325 | 5 |
Sr2AlGaFe2O7 (mvc-13325) | 0.6081 | 0.120 | 5 |
LiCaMgSiN3 (mp-1020108) | 0.5919 | 0.000 | 5 |
Si (mp-644693) | 0.7376 | 0.412 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Li_sv Ge_d O |
Final Energy/Atom-5.4260 eV |
Corrected Energy-413.1427 eV
-413.1427 eV = -390.6694 eV (uncorrected energy) - 22.4733 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)