Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.901 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.63 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap4.963 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 50.7 |
LaAlO3 (mp-2920) | <1 0 0> | <0 1 0> | 146.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 1 1> | 152.2 |
LaAlO3 (mp-2920) | <1 1 1> | <0 1 1> | 253.7 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 50.7 |
AlN (mp-661) | <1 0 0> | <0 1 -1> | 217.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 196.2 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 195.2 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 142.8 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 146.4 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 253.7 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 244.0 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 341.6 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 240.0 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 292.8 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 300.0 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 146.4 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 244.0 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 153.6 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 195.2 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 244.0 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 48.8 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 274.7 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 244.0 |
KCl (mp-23193) | <1 1 0> | <1 1 1> | 233.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 274.7 |
TePb (mp-19717) | <1 0 0> | <0 1 1> | 253.7 |
TePb (mp-19717) | <1 1 0> | <0 1 1> | 304.4 |
TePb (mp-19717) | <1 1 1> | <0 1 1> | 152.2 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 244.0 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 1> | 304.4 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 1> | 304.4 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 274.7 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 274.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 274.7 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 180.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 196.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 292.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 311.0 |
BN (mp-984) | <0 0 1> | <0 1 1> | 203.0 |
BN (mp-984) | <1 0 0> | <1 0 1> | 214.2 |
BN (mp-984) | <1 0 1> | <1 1 -1> | 281.8 |
BN (mp-984) | <1 1 0> | <0 0 1> | 274.7 |
BN (mp-984) | <1 1 1> | <0 0 1> | 274.7 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 142.8 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 353.2 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 157.0 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 196.2 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 311.0 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 196.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr2Ag2O7 (mp-504441) | 0.5588 | 0.020 | 3 |
Na2S2O7 (mp-31269) | 0.5198 | 0.000 | 3 |
NaAsO3 (mp-17868) | 0.5658 | 0.002 | 3 |
Na5P3O10 (mp-557529) | 0.5363 | 0.005 | 3 |
Na2Cr2O7 (mp-704459) | 0.5707 | 0.000 | 3 |
Li4Mn(PO3)6 (mp-861540) | 0.3706 | 0.168 | 4 |
Li4Ni(PO3)6 (mp-863893) | 0.3975 | 0.106 | 4 |
Li4V(PO3)6 (mp-763530) | 0.3735 | 0.124 | 4 |
Li4Mn5(P3O11)2 (mp-540032) | 0.4403 | 0.032 | 4 |
Li4Fe(PO3)6 (mp-761457) | 0.3845 | 0.126 | 4 |
Li2Mn2P2O7F2 (mp-770546) | 0.5815 | 0.095 | 5 |
KNaZnP2O7 (mp-554157) | 0.5995 | 0.000 | 5 |
SrZnCo(PO4)2 (mvc-2988) | 0.6154 | 0.022 | 5 |
BaNaEu(SiO3)3 (mp-1019735) | 0.5483 | 0.000 | 5 |
BaNaNd(SiO3)3 (mp-13791) | 0.5588 | 0.002 | 5 |
InBP2H5NO9 (mp-752709) | 0.7037 | 0.000 | 6 |
FeBP2H5NO9 (mp-766957) | 0.7105 | 0.100 | 6 |
Na2Gd2MgSi4(O6F)2 (mp-557538) | 0.6692 | 0.000 | 6 |
NaInBP2HO9 (mp-757312) | 0.7322 | 0.013 | 6 |
AlBP2H5NO9 (mp-24757) | 0.6774 | 0.000 | 6 |
Ca2Al2FeSi4BHO16 (mp-540713) | 0.7487 | 0.068 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Na_pv Ca_sv P O |
Final Energy/Atom-6.6656 eV |
Corrected Energy-169.5929 eV
Uncorrected energy = -159.9749 eV
Composition-based energy adjustment (-0.687 eV/atom x 14.0 atoms) = -9.6180 eV
Corrected energy = -169.5929 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)