Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.132 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.146 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.25 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.241 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4c2 [116] |
HallP 4 2c |
Point Group42m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 214.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 348.6 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 227.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 348.6 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 217.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 305.0 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 322.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 174.3 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 227.9 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 227.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 227.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 348.6 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 322.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 217.9 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 268.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 43.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 87.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 305.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 261.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 174.3 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 227.9 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 268.6 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 207.5 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 227.9 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 175.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 227.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 227.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 348.6 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 161.2 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 227.9 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 217.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 268.6 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 303.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 348.6 |
BN (mp-984) | <0 0 1> | <1 0 0> | 214.9 |
BN (mp-984) | <1 0 0> | <1 0 0> | 268.6 |
BN (mp-984) | <1 0 1> | <1 0 0> | 161.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 0> | 303.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 348.6 |
Al (mp-134) | <1 0 0> | <1 0 0> | 161.2 |
Al (mp-134) | <1 1 0> | <1 1 0> | 227.9 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 227.9 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 130.7 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 268.6 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 107.4 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 0> | 227.9 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 305.0 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 43.6 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 303.9 |
TeO2 (mp-2125) | <1 1 0> | <1 1 0> | 303.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | -0.02392 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.02392 | 0.00000 | 0.00000 |
-0.11475 | 0.11475 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.16228 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
0.00000 |
1.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.25 | 0.00 | 0.00 |
0.00 | 2.25 | 0.00 |
0.00 | 0.00 | 2.33 |
Dielectric Tensor εij (total) |
||
---|---|---|
4.14 | 0.00 | 0.00 |
0.00 | 4.14 | 0.00 |
0.00 | 0.00 | 4.72 |
Polycrystalline dielectric constant
εpoly∞
2.28
|
Polycrystalline dielectric constant
εpoly
4.33
|
Refractive Index n1.51 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AsAuO3 (mp-755240) | 0.5959 | 0.117 | 3 |
VBO4 (mp-771386) | 0.5772 | 0.068 | 3 |
AlPO4 (mp-560815) | 0.5166 | 0.030 | 3 |
AlPO4 (mp-667310) | 0.6466 | 0.022 | 3 |
CoPO4 (mp-694829) | 0.6634 | 0.196 | 3 |
RbAlSiO4 (mp-6434) | 0.6104 | 0.000 | 4 |
CsSi3HO7 (mp-758180) | 0.6267 | 0.002 | 4 |
CsLiCrO4 (mp-615884) | 0.6211 | 0.000 | 4 |
CsFeSiO4 (mp-644325) | 0.6110 | 0.000 | 4 |
KBePO4 (mp-7324) | 0.5789 | 0.000 | 4 |
Si2O5 (mp-862998) | 0.3503 | 0.593 | 2 |
SiO2 (mp-553993) | 0.4578 | 0.039 | 2 |
SiO2 (mp-556464) | 0.4692 | 0.240 | 2 |
SiO2 (mp-600026) | 0.4619 | 0.050 | 2 |
SiO2 (mp-556662) | 0.3892 | 0.070 | 2 |
RbB2P2HO9 (mp-758281) | 0.7305 | 0.000 | 5 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.7702 eV |
Corrected Energy-197.7203 eV
-197.7203 eV = -186.4837 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)