Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.588 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.039 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 228.0 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 126.2 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 178.4 |
AlN (mp-661) | <1 0 0> | <1 0 -1> | 172.4 |
CeO2 (mp-20194) | <1 1 0> | <1 1 -1> | 291.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 228.0 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 318.9 |
GaAs (mp-2534) | <1 0 0> | <1 1 -1> | 291.0 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 208.7 |
SiO2 (mp-6930) | <0 0 1> | <1 0 -1> | 172.4 |
SiO2 (mp-6930) | <1 0 1> | <1 1 1> | 247.9 |
SiO2 (mp-6930) | <1 1 0> | <1 1 -1> | 145.5 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 252.4 |
GaN (mp-804) | <1 0 1> | <1 1 -1> | 291.0 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 273.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 267.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 1> | 247.9 |
ZnSe (mp-1190) | <1 0 0> | <1 1 -1> | 291.0 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 267.5 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 312.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 223.2 |
CdS (mp-672) | <0 0 1> | <0 1 1> | 315.5 |
CdS (mp-672) | <1 0 0> | <1 0 -1> | 57.5 |
CdS (mp-672) | <1 0 1> | <1 1 -1> | 291.0 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 287.4 |
Te2W (mp-22693) | <0 0 1> | <1 1 -1> | 218.2 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 165.3 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 228.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 208.7 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 44.6 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 182.4 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 223.2 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 273.6 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 228.0 |
Te2Mo (mp-602) | <1 1 1> | <1 0 -1> | 287.4 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 89.3 |
BN (mp-984) | <1 0 1> | <0 1 0> | 267.5 |
BN (mp-984) | <1 1 1> | <0 1 0> | 178.4 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 223.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 1> | 315.5 |
BN (mp-984) | <0 0 1> | <1 1 0> | 191.3 |
BN (mp-984) | <1 0 0> | <1 0 0> | 228.0 |
LiNbO3 (mp-3731) | <1 0 1> | <1 1 0> | 318.9 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 315.5 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 133.8 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 178.4 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 223.0 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 312.5 |
CdTe (mp-406) | <1 1 1> | <1 0 0> | 228.0 |
TeO2 (mp-2125) | <0 1 1> | <1 0 -1> | 229.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TiOF (mp-752496) | 0.1598 | 0.096 | 3 |
TaNO (mp-4165) | 0.2908 | 0.000 | 3 |
VOF (mp-768037) | 0.2945 | 0.012 | 3 |
NbNO (mp-781710) | 0.3473 | 0.025 | 3 |
NbNO (mp-7596) | 0.3415 | 0.000 | 3 |
HfO2 (mp-775757) | 0.3894 | 0.010 | 2 |
NbO2 (mp-776975) | 0.3272 | 0.072 | 2 |
ZrO2 (mp-776404) | 0.3812 | 0.009 | 2 |
CeSe2 (mp-1080303) | 0.2347 | 0.024 | 2 |
CeSe2 (mp-1080853) | 0.2666 | 0.029 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Dy_3 S Cl |
Final Energy/Atom-5.6992 eV |
Corrected Energy-72.8588 eV
Uncorrected energy = -68.3908 eV
Composition-based energy adjustment (-0.503 eV/atom x 4.0 atoms) = -2.0120 eV
Composition-based energy adjustment (-0.614 eV/atom x 4.0 atoms) = -2.4560 eV
Corrected energy = -72.8588 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)