material

Rb2NiF4

ID:

mp-561317

DOI:

10.17188/1271995


Tags: High pressure experimental phase Dirubidium tetrafluoroniccolate

Material Details

Final Magnetic Moment
2.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-2.642 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.23 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
4.528 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal
We have not yet calculated a detailed bandstructure for this material

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ag (mp-124) <1 0 0> <0 0 1> 0.000 17.3
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.000 86.6
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.001 163.2
TePb (mp-19717) <1 0 0> <0 0 1> 0.004 86.6
PbSe (mp-2201) <1 0 0> <0 0 1> 0.006 155.8
GaN (mp-804) <0 0 1> <1 0 1> 0.007 241.0
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.007 155.8
Au (mp-81) <1 0 0> <0 0 1> 0.007 17.3
GaSe (mp-1943) <0 0 1> <1 0 1> 0.008 241.0
AlN (mp-661) <1 0 0> <1 1 1> 0.010 250.2
LiTaO3 (mp-3666) <1 0 0> <1 0 0> 0.012 288.5
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.012 138.5
GaSb (mp-1156) <1 0 0> <0 0 1> 0.014 155.8
LaF3 (mp-905) <0 0 1> <1 0 1> 0.015 180.7
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.016 225.0
SiC (mp-7631) <1 0 1> <1 0 0> 0.017 288.5
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.017 230.8
Cu (mp-30) <1 1 1> <0 0 1> 0.018 363.5
AlN (mp-661) <1 1 1> <0 0 1> 0.019 311.6
CdSe (mp-2691) <1 0 0> <0 0 1> 0.023 155.8
Fe2O3 (mp-24972) <1 1 0> <1 1 0> 0.026 244.8
Fe2O3 (mp-24972) <0 0 1> <0 0 1> 0.027 363.5
Ge3(BiO3)4 (mp-23560) <1 0 0> <0 0 1> 0.031 225.0
Bi2Se3 (mp-541837) <0 0 1> <1 0 1> 0.031 60.2
C (mp-66) <1 1 0> <1 0 1> 0.032 180.7
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.032 86.6
SiC (mp-11714) <1 0 1> <0 0 1> 0.035 259.7
Mg (mp-153) <1 0 1> <0 0 1> 0.037 207.7
WS2 (mp-224) <0 0 1> <1 0 1> 0.037 241.0
MoS2 (mp-1434) <0 0 1> <1 0 1> 0.038 241.0
GaN (mp-804) <1 0 1> <0 0 1> 0.039 207.7
TiO2 (mp-2657) <1 1 0> <0 0 1> 0.040 155.8
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.043 138.5
Y3Fe5O12 (mp-19648) <1 0 0> <0 0 1> 0.044 155.8
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.048 138.5
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.052 155.8
TiO2 (mp-390) <1 0 0> <0 0 1> 0.052 259.7
GaN (mp-804) <1 1 1> <0 0 1> 0.053 277.0
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.058 311.6
SiC (mp-8062) <1 0 0> <0 0 1> 0.064 155.8
ZnO (mp-2133) <0 0 1> <0 0 1> 0.064 346.2
CdS (mp-672) <1 1 0> <1 0 1> 0.065 301.2
CdTe (mp-406) <1 0 0> <0 0 1> 0.067 86.6
Fe2O3 (mp-24972) <1 0 0> <1 0 0> 0.070 288.5
WS2 (mp-224) <1 1 1> <1 0 1> 0.071 241.0
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.072 155.8
CdS (mp-672) <1 0 0> <1 0 0> 0.076 57.7
InSb (mp-20012) <1 0 0> <0 0 1> 0.079 86.6
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.079 311.6
LaAlO3 (mp-2920) <1 0 0> <1 0 0> 0.081 288.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
79 26 24 0 0 0
26 79 24 0 0 0
24 24 67 0 0 0
0 0 0 14 0 0
0 0 0 0 14 0
0 0 0 0 0 28
Compliance Tensor Sij (10-12Pa-1)
15.3 -4 -4 0 0 0
-4 15.3 -4 0 0 0
-4 -4 17.8 0 0 0
0 0 0 73.2 0 0
0 0 0 0 73.2 0
0 0 0 0 0 35.8
Shear Modulus GV
21 GPa
Bulk Modulus KV
41 GPa
Shear Modulus GR
19 GPa
Bulk Modulus KR
41 GPa
Shear Modulus GVRH
20 GPa
Bulk Modulus KVRH
41 GPa
Elastic Anisotropy
0.54
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Nd2AlNO3 (mp-546679) 0.6128 0.076 4
Eu2AlNO3 (mp-1025206) 0.5632 0.119 4
Rb2Cr(BrCl)2 (mp-1025321) 0.3567 0.000 4
Ce2AlNO3 (mp-1025275) 0.5292 0.099 4
Pr2AlNO3 (mp-1025277) 0.6025 0.071 4
SnF4 (mp-2706) 0.6878 0.000 2
Rb2CoF4 (mp-559959) 0.0704 0.083 3
K4I2O (mp-768368) 0.0309 0.000 3
Cs2CaF4 (mp-15157) 0.0944 0.000 3
K2MgH4 (mp-23956) 0.0999 0.000 3
K2MgF4 (mp-31212) 0.0858 0.000 3
SrLiLa3MnO8 (mp-779988) 0.7399 0.015 5
Sr5La5Cu(NiO5)4 (mp-690554) 0.6421 0.000 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA+U
Energy Cutoff
520 eV
# of K-points
None
U Values
Ni: 6.2 eV
Pseudopotentials
VASP PAW: Rb_sv Ni_pv F
Final Energy/Atom
-4.2475 eV
Corrected Energy
-31.8967 eV
-31.8967 eV = -29.7327 eV (uncorrected energy) - 2.1640 eV (MP Advanced Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 69682
Submitted by
User remarks:
  • High pressure experimental phase
  • Dirubidium tetrafluoroniccolate

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)