Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.266 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.012 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density1.80 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSiO2 |
Band Gap5.451 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPmmn [59] |
HallP 2 2ab 1ab |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 301.4 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 301.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 301.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 180.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 241.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 180.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 180.8 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 116.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 60.3 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 180.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 180.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 180.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 301.4 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 301.4 |
Al (mp-134) | <1 1 0> | <0 0 1> | 180.8 |
TeO2 (mp-2125) | <0 1 1> | <0 0 1> | 301.4 |
TeO2 (mp-2125) | <1 0 1> | <0 0 1> | 301.4 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 116.7 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 241.1 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 301.4 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 301.4 |
TiO2 (mp-2657) | <1 1 1> | <0 1 1> | 262.6 |
MgO (mp-1265) | <1 1 0> | <0 1 0> | 233.3 |
GdScO3 (mp-5690) | <1 0 0> | <0 0 1> | 180.8 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 116.7 |
Mg (mp-153) | <1 1 0> | <0 1 0> | 116.7 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 180.8 |
Ni (mp-23) | <1 1 0> | <0 1 1> | 262.6 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 180.8 |
SiC (mp-11714) | <0 0 1> | <0 1 0> | 116.7 |
NdGaO3 (mp-3196) | <1 0 0> | <0 0 1> | 180.8 |
SiC (mp-11714) | <1 1 0> | <0 1 1> | 262.6 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 180.8 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 180.8 |
NaCl (mp-22862) | <1 1 0> | <0 0 1> | 180.8 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 180.8 |
ZrO2 (mp-2858) | <1 0 1> | <0 1 1> | 131.3 |
YAlO3 (mp-3792) | <0 1 1> | <0 0 1> | 241.1 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 120.6 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 301.4 |
ZrO2 (mp-2858) | <0 1 0> | <0 0 1> | 301.4 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 116.7 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 301.4 |
CdWO4 (mp-19387) | <1 1 1> | <0 0 1> | 301.4 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 301.4 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 0> | 116.7 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 241.1 |
TiO2 (mp-390) | <1 0 1> | <0 0 1> | 120.6 |
SiC (mp-8062) | <1 1 0> | <0 0 1> | 241.1 |
SiC (mp-8062) | <1 1 1> | <0 1 0> | 233.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
AlPO4 (mp-37990) | 0.4125 | 0.014 | 3 |
AlPO4 (mp-557842) | 0.3846 | 0.011 | 3 |
AlPO4 (mp-558056) | 0.3945 | 0.011 | 3 |
AlPO4 (mp-675254) | 0.4207 | 0.012 | 3 |
AlPO4 (mp-1019510) | 0.4157 | 0.010 | 3 |
RbAlSiO4 (mp-6434) | 0.7486 | 0.000 | 4 |
CsAlSiO4 (mp-561457) | 0.6665 | 0.000 | 4 |
CsBePO4 (mp-15395) | 0.5680 | 0.000 | 4 |
SiO2 (mp-600037) | 0.1703 | 0.018 | 2 |
SiO2 (mp-653763) | 0.1536 | 0.017 | 2 |
CrN2 (mp-1096968) | 0.1683 | 0.360 | 2 |
CrN2 (mp-1096961) | 0.1795 | 0.373 | 2 |
CrN2 (mp-1097059) | 0.1752 | 0.359 | 2 |
Explore more synthesis descriptions for materials of composition SiO2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Si O |
Final Energy/Atom-7.9042 eV |