Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.526 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.044 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.40 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCr5O12 + O2 |
Band Gap2.308 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinAma2 [40] |
HallA 2 2a |
Point Groupmm2 |
Crystal Systemorthorhombic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 1> | 308.0 |
GaTe (mp-542812) | <0 0 1> | <0 0 1> | 237.8 |
SiC (mp-8062) | <1 0 0> | <1 1 0> | 287.1 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 1> | 55.9 |
TiO2 (mp-2657) | <0 0 1> | <1 1 0> | 215.3 |
Te2Mo (mp-602) | <1 1 1> | <1 1 0> | 287.1 |
Fe2O3 (mp-24972) | <1 0 0> | <0 1 0> | 142.0 |
Fe2O3 (mp-24972) | <1 0 1> | <0 0 1> | 148.6 |
SiC (mp-11714) | <1 0 0> | <0 1 0> | 94.7 |
YAlO3 (mp-3792) | <1 1 1> | <0 1 0> | 189.3 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 267.5 |
Te2Mo (mp-602) | <1 0 1> | <0 1 0> | 331.3 |
CeO2 (mp-20194) | <1 1 0> | <0 1 1> | 167.7 |
TiO2 (mp-2657) | <1 0 1> | <0 1 1> | 279.4 |
Si (mp-149) | <1 1 0> | <0 1 1> | 167.7 |
Mg (mp-153) | <0 0 1> | <0 1 1> | 279.4 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 267.5 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 267.5 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 279.4 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 89.2 |
CdWO4 (mp-19387) | <0 1 1> | <0 1 0> | 284.0 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 208.1 |
C (mp-66) | <1 1 1> | <0 0 1> | 89.2 |
Cu (mp-30) | <1 1 0> | <0 1 1> | 55.9 |
MoS2 (mp-1434) | <0 0 1> | <0 1 1> | 279.4 |
WS2 (mp-224) | <0 0 1> | <0 1 1> | 279.4 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 208.1 |
Si (mp-149) | <1 1 1> | <0 0 1> | 208.1 |
CdWO4 (mp-19387) | <0 1 0> | <0 0 1> | 237.8 |
Au (mp-81) | <1 1 1> | <0 1 1> | 335.3 |
MgF2 (mp-1249) | <1 0 0> | <0 1 0> | 142.0 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 142.0 |
ZnO (mp-2133) | <1 0 1> | <1 1 0> | 215.3 |
TiO2 (mp-390) | <1 1 0> | <1 0 1> | 308.0 |
Te2Mo (mp-602) | <1 1 0> | <1 1 0> | 287.1 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 267.5 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 55.9 |
BN (mp-984) | <1 0 1> | <0 1 1> | 223.6 |
GdScO3 (mp-5690) | <1 0 0> | <1 0 1> | 184.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 47.3 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 284.0 |
NdGaO3 (mp-3196) | <0 1 0> | <0 1 1> | 167.7 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 267.5 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 287.1 |
GaP (mp-2490) | <1 1 0> | <0 1 1> | 167.7 |
Ag (mp-124) | <1 1 1> | <0 1 1> | 335.3 |
LiTaO3 (mp-3666) | <1 0 0> | <0 1 0> | 142.0 |
BaTiO3 (mp-5986) | <1 0 1> | <0 0 1> | 118.9 |
GdScO3 (mp-5690) | <0 0 1> | <1 0 0> | 161.9 |
GaTe (mp-542812) | <1 0 0> | <0 1 1> | 223.6 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
77 | 6 | 2 | 0 | 0 | 0 |
6 | 7 | 2 | 0 | 0 | 0 |
2 | 2 | 9 | 0 | 0 | 0 |
0 | 0 | 0 | 1 | 0 | 0 |
0 | 0 | 0 | 0 | 3 | 0 |
0 | 0 | 0 | 0 | 0 | 7 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
13.9 | -10.8 | -1.3 | 0 | 0 | 0 |
-10.8 | 157.2 | -26.6 | 0 | 0 | 0 |
-1.3 | -26.6 | 118.6 | 0 | 0 | 0 |
0 | 0 | 0 | 792.3 | 0 | 0 |
0 | 0 | 0 | 0 | 349.1 | 0 |
0 | 0 | 0 | 0 | 0 | 147.9 |
Shear Modulus GV8 GPa |
Bulk Modulus KV12 GPa |
Shear Modulus GR3 GPa |
Bulk Modulus KR5 GPa |
Shear Modulus GVRH5 GPa |
Bulk Modulus KVRH9 GPa |
Elastic Anisotropy9.95 |
Poisson's Ratio0.24 |
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.23945 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00375 | 0.00000 | 0.00000 |
0.11470 | -0.01923 | 0.82744 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.83557 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
1.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
5.05 | 0.00 | 0.00 |
0.00 | 5.43 | 0.00 |
0.00 | 0.00 | 2.69 |
Dielectric Tensor εij (total) |
||
---|---|---|
12.81 | 0.00 | 0.00 |
0.00 | 5.47 | 0.00 |
0.00 | 0.00 | 3.03 |
Polycrystalline dielectric constant
εpoly∞
4.39
|
Polycrystalline dielectric constant
εpoly
7.10
|
Refractive Index n2.09 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V2SO8 (mp-770164) | 0.3859 | 0.068 | 3 |
PNF2 (mp-555292) | 0.4659 | 0.004 | 3 |
Si2H2O3 (mp-24431) | 0.4027 | 0.023 | 3 |
Si2H6O (mp-27949) | 0.3225 | 0.050 | 3 |
Si3(Cl4O)2 (mp-30224) | 0.3694 | 0.008 | 3 |
TcH4NO4 (mp-23925) | 0.5554 | 0.028 | 4 |
ReH4NO4 (mp-24128) | 0.6005 | 0.000 | 4 |
P2NCl5O (mp-559917) | 0.4491 | 0.016 | 4 |
BeP2(HO)4 (mp-695815) | 0.4426 | 0.026 | 4 |
FeN3ClO3 (mp-566054) | 0.6517 | 0.646 | 4 |
V2O5 (mp-775847) | 0.5518 | 0.011 | 2 |
CrO3 (mp-779941) | 0.2190 | 0.075 | 2 |
V2O5 (mp-776344) | 0.3814 | 0.012 | 2 |
CrO3 (mp-772550) | 0.3160 | 0.058 | 2 |
CrO3 (mp-715566) | 0.2149 | 0.054 | 2 |
FeBN3O3F4 (mp-631397) | 0.6440 | 0.417 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Cr_pv O |
Final Energy/Atom-6.6204 eV |
Corrected Energy-61.2033 eV
-61.2033 eV = -52.9635 eV (uncorrected energy) - 4.2137 eV (MP Anion Correction) - 4.0260 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)