Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.508 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.056 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.27 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToK4Th(MoO4)4 + Th(MoO4)2 |
Band Gap2.839 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 201.6 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 202.0 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 201.6 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 268.9 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 134.4 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 268.9 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 268.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 268.9 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 268.9 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 242.7 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 201.6 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 202.0 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 201.6 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 0> | 201.6 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 201.6 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 201.6 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 134.4 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 268.9 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 202.0 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 134.4 |
LiGaO2 (mp-5854) | <1 1 1> | <1 0 0> | 268.9 |
TeO2 (mp-2125) | <0 1 0> | <1 0 0> | 67.2 |
PbS (mp-21276) | <1 1 0> | <1 0 0> | 201.6 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 268.9 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 201.6 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 268.9 |
MgO (mp-1265) | <1 1 0> | <1 0 0> | 201.6 |
NdGaO3 (mp-3196) | <0 0 1> | <1 0 0> | 268.9 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 0> | 268.9 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 268.9 |
C (mp-66) | <1 1 0> | <1 0 0> | 201.6 |
Mg (mp-153) | <1 1 0> | <1 0 0> | 201.6 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 268.9 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 201.6 |
Si (mp-149) | <1 0 0> | <1 0 0> | 268.9 |
Au (mp-81) | <1 1 0> | <1 0 0> | 201.6 |
WS2 (mp-224) | <1 1 1> | <1 1 0> | 242.7 |
C (mp-48) | <1 0 1> | <1 0 0> | 201.6 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 134.4 |
ZrO2 (mp-2858) | <1 0 0> | <1 0 0> | 201.6 |
YAlO3 (mp-3792) | <0 0 1> | <1 0 0> | 201.6 |
YAlO3 (mp-3792) | <1 0 0> | <1 0 0> | 201.6 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 268.9 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 268.9 |
WS2 (mp-224) | <0 0 1> | <0 1 0> | 202.0 |
WSe2 (mp-1821) | <1 0 0> | <1 0 0> | 201.6 |
NaCl (mp-22862) | <1 1 0> | <1 0 0> | 134.4 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 0> | 201.6 |
TiO2 (mp-390) | <1 1 0> | <1 0 0> | 268.9 |
CsI (mp-614603) | <1 1 0> | <1 0 0> | 268.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba7(Fe3S7)2 (mp-672715) | 0.6650 | 0.236 | 3 |
Cs3HgCl5 (mp-27354) | 0.7161 | 0.001 | 3 |
NaI3O8 (mp-559065) | 0.6343 | 0.000 | 3 |
La2(MoO4)3 (mp-578938) | 0.6949 | 0.000 | 3 |
Bi2(MoO4)3 (mp-32039) | 0.6741 | 0.000 | 3 |
LiY(MoO4)2 (mp-866387) | 0.6029 | 0.076 | 4 |
CsDy(MoO4)2 (mp-622861) | 0.6229 | 0.000 | 4 |
K2Th(MoO4)3 (mp-566934) | 0.6529 | 0.011 | 4 |
RbBi(MoO4)2 (mp-600262) | 0.6330 | 0.000 | 4 |
CsY(MoO4)2 (mp-1096960) | 0.6431 | 0.026 | 4 |
KHo2Cu(MoO4)4 (mp-699660) | 0.7412 | 0.028 | 5 |
Ba4LaGe3SbSe13 (mp-683936) | 0.7340 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMo: 4.38 eV |
PseudopotentialsVASP PAW: K_sv Th Mo_pv O |
Final Energy/Atom-7.0925 eV |
Corrected Energy-293.3693 eV
-293.3693 eV = -255.3283 eV (uncorrected energy) - 21.1860 eV (MP Advanced Correction) - 16.8550 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)