Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.493 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.44 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.017 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <1 -1 -1> | 281.5 |
AlN (mp-661) | <1 0 1> | <1 -1 -1> | 281.5 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 291.9 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 233.5 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 151.6 |
GaN (mp-804) | <1 0 1> | <1 -1 0> | 270.2 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 291.9 |
CdS (mp-672) | <1 0 0> | <1 -1 -1> | 281.5 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 291.9 |
LiF (mp-1138) | <1 1 1> | <1 -1 -1> | 281.5 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 273.6 |
AlN (mp-661) | <1 1 0> | <1 0 -1> | 273.6 |
GaSe (mp-1943) | <0 0 1> | <1 -1 -1> | 187.7 |
BN (mp-984) | <1 0 0> | <0 1 1> | 212.9 |
BN (mp-984) | <1 0 1> | <1 0 -1> | 182.4 |
BN (mp-984) | <1 1 1> | <0 0 1> | 233.5 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 276.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 233.5 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 -1> | 294.0 |
MoS2 (mp-1434) | <0 0 1> | <1 0 -1> | 273.6 |
Al (mp-134) | <1 1 1> | <1 -1 -1> | 281.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 233.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 291.9 |
KTaO3 (mp-3614) | <1 1 1> | <1 -1 -1> | 281.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 233.5 |
LiGaO2 (mp-5854) | <0 1 0> | <1 -1 0> | 270.2 |
TeO2 (mp-2125) | <0 1 0> | <1 -1 0> | 270.2 |
Te2Mo (mp-602) | <0 0 1> | <1 0 -1> | 273.6 |
Te2Mo (mp-602) | <1 0 1> | <1 0 -1> | 273.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 291.9 |
LiTaO3 (mp-3666) | <1 0 0> | <0 0 1> | 291.9 |
LiTaO3 (mp-3666) | <1 0 1> | <0 0 1> | 233.5 |
MgO (mp-1265) | <1 1 1> | <0 1 0> | 252.0 |
Al (mp-134) | <1 0 0> | <0 0 1> | 291.9 |
LiGaO2 (mp-5854) | <1 0 0> | <1 0 0> | 276.4 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 276.4 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 276.4 |
C (mp-66) | <1 1 0> | <0 0 1> | 291.9 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 276.4 |
GdScO3 (mp-5690) | <1 1 1> | <0 1 -1> | 294.0 |
Mg (mp-153) | <0 0 1> | <1 -1 0> | 270.2 |
TbScO3 (mp-31119) | <1 0 0> | <0 0 1> | 233.5 |
TbScO3 (mp-31119) | <1 1 1> | <0 1 -1> | 294.0 |
BaTiO3 (mp-5986) | <1 0 0> | <1 -1 -1> | 187.7 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 291.9 |
NdGaO3 (mp-3196) | <1 0 0> | <1 1 1> | 175.6 |
Ga2O3 (mp-886) | <0 1 0> | <1 -1 -1> | 281.5 |
Ga2O3 (mp-886) | <1 0 0> | <1 -1 0> | 90.1 |
WS2 (mp-224) | <0 0 1> | <1 0 -1> | 273.6 |
WS2 (mp-224) | <1 0 0> | <0 0 1> | 233.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca2CrN2 (mvc-15308) | 0.5914 | 0.076 | 3 |
Rb2PbO2 (mp-504598) | 0.2347 | 0.000 | 3 |
K2SnO2 (mp-752692) | 0.2209 | 0.000 | 3 |
K2PbO2 (mp-556517) | 0.4488 | 0.000 | 3 |
K4Bi2O5 (mp-29542) | 0.5664 | 0.005 | 3 |
Li3VO3F2 (mp-764231) | 0.7499 | 0.112 | 4 |
Na3NbAs2O9 (mp-565593) | 0.7095 | 0.696 | 4 |
TaZnBiO5 (mvc-7449) | 0.7485 | 0.117 | 4 |
Ba2Tl2Zn2Sn3O10 (mvc-2762) | 0.6315 | 0.360 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Pb_d O |
Final Energy/Atom-4.2915 eV |
Corrected Energy-91.3259 eV
Uncorrected energy = -85.8299 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Corrected energy = -91.3259 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)