Final Magnetic Moment0.610 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.567 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.55 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 232.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 186.2 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 182.8 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 154.8 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 232.7 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 232.7 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 231.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 232.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 182.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 243.7 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 154.8 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 309.7 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 232.3 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 154.8 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 232.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 325.8 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 279.3 |
Te2Mo (mp-602) | <1 1 0> | <0 0 1> | 93.1 |
Te2Mo (mp-602) | <1 1 1> | <1 0 0> | 182.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 139.6 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 279.3 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 60.9 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 154.3 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 304.6 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 139.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 232.7 |
BN (mp-984) | <1 0 1> | <0 1 0> | 308.5 |
BN (mp-984) | <1 1 0> | <0 0 1> | 232.7 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 304.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 139.6 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 304.6 |
GaSe (mp-1943) | <1 0 1> | <1 1 1> | 218.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 186.2 |
BN (mp-984) | <0 0 1> | <1 0 0> | 304.6 |
BN (mp-984) | <1 1 1> | <0 1 0> | 231.4 |
Al (mp-134) | <1 0 0> | <1 0 0> | 243.7 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 308.5 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 325.8 |
LiGaO2 (mp-5854) | <1 1 1> | <0 1 0> | 231.4 |
MgO (mp-1265) | <1 0 0> | <1 1 1> | 109.3 |
TiO2 (mp-2657) | <1 0 1> | <0 1 1> | 180.2 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 232.7 |
SiC (mp-7631) | <0 0 1> | <1 0 1> | 232.3 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 182.8 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 182.8 |
SiC (mp-7631) | <1 1 1> | <1 0 0> | 243.7 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 186.2 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 182.8 |
MgO (mp-1265) | <1 1 0> | <1 0 1> | 77.4 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 325.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Eu2SiO4 (mp-504653) | 0.6037 | 0.014 | 3 |
Sr2SiO4 (mp-17825) | 0.5974 | 0.009 | 3 |
Cs2TeO4 (mp-669353) | 0.6623 | 0.000 | 3 |
Rb2MgH4 (mp-643770) | 0.6548 | 0.013 | 3 |
K2ZnCl4 (mp-653454) | 0.6371 | 0.014 | 3 |
K3Gd(PO4)2 (mp-978099) | 0.4458 | 0.000 | 4 |
K3NdV2O8 (mp-19584) | 0.2727 | 0.000 | 4 |
K3Eu(PO4)2 (mp-17089) | 0.4739 | 0.237 | 4 |
K3Nd(PO4)2 (mp-17187) | 0.5020 | 0.000 | 4 |
K3EuV2O8 (mp-630799) | 0.0258 | 0.000 | 4 |
K2UP2(H2O5)2 (mp-722535) | 0.7452 | 0.377 | 5 |
K2USO7F2 (mp-863004) | 0.7414 | 0.185 | 5 |
SrCaP2WO8 (mvc-3024) | 0.6797 | 0.266 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: K_sv Eu V_pv O |
Final Energy/Atom-6.9934 eV |
Corrected Energy-213.6082 eV
Uncorrected energy = -195.8162 eV
Composition-based energy adjustment (-0.687 eV/atom x 16.0 atoms) = -10.9920 eV
Composition-based energy adjustment (-1.700 eV/atom x 4.0 atoms) = -6.8000 eV
Corrected energy = -213.6082 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)