Final Magnetic Moment12.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.397 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.76 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.358 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 1> | 270.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 278.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 71.1 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 333.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 134.1 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 284.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 71.1 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 166.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 284.4 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 333.7 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 278.1 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 270.8 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 278.1 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 333.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 284.4 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 284.4 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 222.5 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 213.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 213.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 134.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 145.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 -1> | 114.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 213.3 |
CdS (mp-672) | <1 0 0> | <1 1 -1> | 253.9 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 284.4 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 134.1 |
LiF (mp-1138) | <1 1 1> | <1 0 -1> | 114.1 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 284.4 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 284.4 |
YVO4 (mp-19133) | <1 0 0> | <0 1 0> | 222.5 |
Te2Mo (mp-602) | <1 1 0> | <0 1 0> | 278.1 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 204.4 |
GaSe (mp-1943) | <1 0 1> | <0 1 1> | 270.8 |
BN (mp-984) | <0 0 1> | <0 1 0> | 333.7 |
BN (mp-984) | <1 0 0> | <1 1 0> | 116.4 |
BN (mp-984) | <1 1 0> | <0 1 0> | 278.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 213.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 71.1 |
Al (mp-134) | <1 1 1> | <1 0 -1> | 114.1 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 222.5 |
SiC (mp-7631) | <1 0 0> | <0 1 0> | 278.1 |
MgO (mp-1265) | <1 1 0> | <0 1 1> | 180.6 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 333.7 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 333.7 |
C (mp-66) | <1 1 0> | <0 1 0> | 333.7 |
GdScO3 (mp-5690) | <0 0 1> | <0 1 0> | 222.5 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 166.9 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 284.4 |
Mg (mp-153) | <1 1 1> | <0 1 0> | 333.7 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 284.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V3(PO4)2 (mp-770844) | 0.3536 | 0.073 | 3 |
Mg3(AsO4)2 (mp-770734) | 0.4286 | 0.065 | 3 |
Mn3(PO4)2 (mp-770563) | 0.2070 | 0.015 | 3 |
Zn3(PO4)2 (mp-553958) | 0.4218 | 0.026 | 3 |
Ni3(PO4)2 (mp-771911) | 0.1422 | 0.192 | 3 |
LiCuPO4 (mp-759627) | 0.4765 | 0.079 | 4 |
CuAgPO4 (mp-608358) | 0.4914 | 0.023 | 4 |
LiCu4(PO4)3 (mp-673145) | 0.4230 | 0.062 | 4 |
LiCoPO4 (mp-761753) | 0.4381 | 0.141 | 4 |
LiCoPO4 (mp-761670) | 0.4890 | 0.081 | 4 |
Bi19O30 (mp-773884) | 0.7355 | 0.050 | 2 |
Bi13O20 (mp-32597) | 0.7427 | 0.033 | 2 |
LiFe3SiPO8 (mp-743761) | 0.6913 | 0.221 | 5 |
Na2Li2V3P2O13 (mp-853239) | 0.6921 | 0.061 | 5 |
NaLiZnP2O7 (mp-676483) | 0.6378 | 0.002 | 5 |
Sr2AlCr2GaO7 (mvc-312) | 0.6115 | 0.186 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesFe: 5.3 eV |
PseudopotentialsVASP PAW: Fe_pv P O |
Final Energy/Atom-7.1667 eV |
Corrected Energy-421.7240 eV
Uncorrected energy = -372.6680 eV
Composition-based energy adjustment (-0.687 eV/atom x 32.0 atoms) = -21.9840 eV
Composition-based energy adjustment (-2.256 eV/atom x 12.0 atoms) = -27.0720 eV
Corrected energy = -421.7240 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)