Final Magnetic Moment0.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.771 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.69 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.953 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI41/a [88] |
HallI 4bw 1bw |
Point Group4/m |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 0 1> | 244.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 352.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 298.5 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 298.5 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 217.1 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 244.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 352.7 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 325.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 135.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 135.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 352.7 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 54.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 325.6 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 325.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 217.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 298.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 244.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 244.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 271.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 162.8 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 298.5 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 244.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 135.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 352.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 81.4 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 135.7 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 298.5 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 135.7 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 217.1 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 135.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 217.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 352.7 |
GaP (mp-2490) | <1 0 0> | <0 0 1> | 244.2 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 135.7 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 189.9 |
LiNbO3 (mp-3731) | <1 0 0> | <0 0 1> | 217.1 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 244.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 135.7 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 108.5 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 325.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 352.7 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 217.1 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 352.7 |
Al (mp-134) | <1 0 0> | <0 0 1> | 135.7 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 217.1 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 352.7 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 325.6 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 135.7 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 135.7 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 325.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaZnCl4 (mp-23522) | 0.4821 | 0.007 | 3 |
NdNbO4 (mp-3901) | 0.5347 | 0.000 | 3 |
YCrO4 (mp-568602) | 0.5402 | 0.026 | 3 |
VBiO4 (mp-559090) | 0.4748 | 0.020 | 3 |
LaNbO4 (mp-542724) | 0.5237 | 0.001 | 3 |
Na4Pu(MoO4)4 (mp-641281) | 0.4786 | 0.021 | 4 |
Na4U(MoO4)4 (mp-567160) | 0.4826 | 0.053 | 4 |
Na4Zr(MoO4)4 (mp-565683) | 0.4614 | 0.004 | 4 |
SmTl(MoO4)2 (mp-19480) | 0.4821 | 0.000 | 4 |
PrTl(MoO4)2 (mp-19490) | 0.4693 | 0.000 | 4 |
TlCl2 (mp-27205) | 0.6247 | 0.000 | 2 |
InI2 (mp-29312) | 0.6865 | 0.000 | 2 |
InBr2 (mp-568108) | 0.6676 | 0.000 | 2 |
GaCl2 (mp-568848) | 0.6668 | 0.000 | 2 |
KF5 (mp-1095521) | 0.6352 | 0.053 | 2 |
Na2YbMoPO8 (mp-579927) | 0.7100 | 0.056 | 5 |
K2YbMoPO8 (mp-565817) | 0.7317 | 0.003 | 5 |
YbZr7Si7PO32 (mp-690946) | 0.7191 | 0.019 | 5 |
NaYPO4F (mp-10804) | 0.6665 | 0.003 | 5 |
NaErPO4F (mp-10935) | 0.6795 | 0.004 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Ca_sv Y_sv As W_pv O |
Final Energy/Atom-7.3982 eV |
Corrected Energy-300.5763 eV
Uncorrected energy = -266.3363 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Composition-based energy adjustment (-4.438 eV/atom x 4.0 atoms) = -17.7520 eV
Corrected energy = -300.5763 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)