Final Magnetic Moment19.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.927 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.190 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.85 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMn2TeO6 + Mn2Te3O8 + Na4Mn2O5 |
Band Gap0.080 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 0 0> | 107.8 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 107.8 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 107.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 107.8 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 138.2 |
TePb (mp-19717) | <1 0 0> | <1 1 1> | 175.3 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 179.9 |
GaSe (mp-1943) | <0 0 1> | <1 1 0> | 150.4 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 90.0 |
TeO2 (mp-2125) | <0 1 1> | <1 1 0> | 150.4 |
TeO2 (mp-2125) | <1 0 1> | <1 1 0> | 150.4 |
SiC (mp-7631) | <1 0 0> | <0 1 1> | 138.2 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 90.0 |
TiO2 (mp-2657) | <1 0 0> | <0 1 1> | 138.2 |
TbScO3 (mp-31119) | <1 0 1> | <1 0 0> | 107.8 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 104.9 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 90.0 |
NdGaO3 (mp-3196) | <1 0 1> | <0 1 0> | 104.9 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 107.8 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 104.9 |
Ga2O3 (mp-886) | <1 0 1> | <0 1 1> | 138.2 |
C (mp-48) | <1 0 0> | <0 0 1> | 269.9 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 107.8 |
NdGaO3 (mp-3196) | <0 1 1> | <0 1 0> | 104.9 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 107.8 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 90.0 |
MgF2 (mp-1249) | <1 0 1> | <0 1 0> | 104.9 |
ZnO (mp-2133) | <0 0 1> | <1 1 0> | 150.4 |
SrTiO3 (mp-4651) | <1 0 1> | <1 0 0> | 107.8 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 215.6 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 269.9 |
Al2O3 (mp-1143) | <1 0 1> | <0 0 1> | 269.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn(FeO2)2 (mvc-15076) | 0.4291 | 0.552 | 3 |
MgAl2O4 (mp-5857) | 0.3940 | 0.099 | 3 |
Mg(FeO2)2 (mvc-14378) | 0.4426 | 0.510 | 3 |
Na(BiO2)2 (mp-777268) | 0.4015 | 0.079 | 3 |
Mg(FeO2)2 (mvc-15084) | 0.4594 | 0.469 | 3 |
Ca5Sc2(CoO6)2 (mvc-13126) | 0.6711 | 0.013 | 4 |
Ca5Mn2(NiO6)2 (mvc-13112) | 0.6482 | 0.106 | 4 |
Ca2MnNiO6 (mvc-10906) | 0.6707 | 0.317 | 4 |
FeBiSbS4 (mp-601716) | 0.6837 | 0.170 | 4 |
CaPr(WO3)2 (mvc-9663) | 0.6944 | 0.208 | 4 |
SrLaTaMnO6 (mp-705452) | 0.7291 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Na_pv Mn_pv Te O |
Final Energy/Atom-6.2649 eV |
Corrected Energy-585.9121 eV
Uncorrected energy = -526.2481 eV
Composition-based energy adjustment (-0.687 eV/atom x 48.0 atoms) = -32.9760 eV
Composition-based energy adjustment (-1.668 eV/atom x 16.0 atoms) = -26.6880 eV
Corrected energy = -585.9121 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)