Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.849 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.118 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.69 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnPO4 + Sr2P2O7 |
Band Gap0.132 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <0 0 1> | 234.2 |
AlN (mp-661) | <1 1 1> | <1 1 1> | 198.1 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 281.0 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 234.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 327.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 327.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 327.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 327.9 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 327.9 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 327.9 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 187.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 281.0 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 140.5 |
CdS (mp-672) | <1 1 0> | <1 0 1> | 149.9 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 327.9 |
GaSe (mp-1943) | <1 1 0> | <0 0 1> | 234.2 |
GaSe (mp-1943) | <1 1 1> | <0 0 1> | 234.2 |
BN (mp-984) | <0 0 1> | <0 0 1> | 327.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 134.9 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 234.2 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 187.0 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 187.3 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 187.3 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 187.3 |
C (mp-66) | <1 1 1> | <0 0 1> | 327.9 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 281.0 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 140.5 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 140.5 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 281.0 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 0 1> | 234.2 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 234.2 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 1> | 149.9 |
InSb (mp-20012) | <1 1 0> | <0 0 1> | 187.3 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 1> | 149.9 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 327.9 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 140.5 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 281.0 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 234.2 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 140.5 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 187.3 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 327.9 |
SiC (mp-11714) | <1 0 1> | <0 0 1> | 234.2 |
C (mp-48) | <0 0 1> | <0 0 1> | 281.0 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 234.2 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 281.0 |
Ga2O3 (mp-886) | <1 0 -1> | <0 0 1> | 187.3 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 327.9 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 140.5 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 234.2 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 327.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SbP2O7 (mp-25896) | 0.6316 | 0.128 | 3 |
Na2S2O7 (mp-31269) | 0.5720 | 0.000 | 3 |
K5As3O10 (mp-27674) | 0.6155 | 0.000 | 3 |
Na2Cr2O7 (mp-704459) | 0.6369 | 0.000 | 3 |
Hg2P2O7 (mp-28455) | 0.5989 | 0.000 | 3 |
Li4Ni(PO3)6 (mp-863893) | 0.5260 | 0.106 | 4 |
BaCa2(SiO3)3 (mp-18216) | 0.5057 | 0.006 | 4 |
MoP3Pb2O11 (mp-567152) | 0.5300 | 0.000 | 4 |
VAg2(PO4)2 (mp-19478) | 0.5268 | 0.071 | 4 |
K2Na3P3O10 (mp-1019781) | 0.4895 | 0.000 | 4 |
LiVSO4F3 (mp-768092) | 0.6243 | 0.056 | 5 |
K2MnSO4F3 (mp-18838) | 0.6255 | 0.000 | 5 |
BaNaEu(SiO3)3 (mp-1019735) | 0.5854 | 0.000 | 5 |
BaNaNd(SiO3)3 (mp-13791) | 0.6186 | 0.002 | 5 |
Rb2MnSO4F3 (mp-19488) | 0.5521 | 0.000 | 5 |
NaInBP2HO9 (mp-757312) | 0.6118 | 0.013 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Sr_sv Mn_pv P O |
Final Energy/Atom-7.1906 eV |
Corrected Energy-526.5835 eV
-526.5835 eV = -488.9593 eV (uncorrected energy) - 30.9008 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)