Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.898 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.19 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.497 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdS (mp-672) | <1 0 0> | <0 1 0> | 313.7 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 251.0 |
LiF (mp-1138) | <1 0 0> | <0 1 1> | 266.4 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 188.2 |
YVO4 (mp-19133) | <0 0 1> | <0 1 0> | 251.0 |
TePb (mp-19717) | <1 1 0> | <0 1 1> | 177.6 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 313.7 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 266.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 313.7 |
BN (mp-984) | <0 0 1> | <0 1 0> | 313.7 |
BN (mp-984) | <1 0 0> | <0 1 1> | 177.6 |
BN (mp-984) | <1 0 1> | <0 1 1> | 177.6 |
BN (mp-984) | <1 1 0> | <0 1 0> | 313.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 1 0> | 313.7 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 313.7 |
Al (mp-134) | <1 1 0> | <0 1 0> | 313.7 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 188.2 |
CdTe (mp-406) | <1 1 0> | <0 1 1> | 177.6 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 251.0 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 267.6 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 267.6 |
TeO2 (mp-2125) | <1 1 0> | <0 1 0> | 188.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 125.7 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 313.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 63.4 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 89.3 |
SiC (mp-7631) | <1 0 1> | <0 1 0> | 251.0 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 313.7 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 251.0 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 313.7 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 313.7 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 177.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 89.2 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 88.8 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 313.7 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 313.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 62.7 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 313.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 63.4 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 89.2 |
C (mp-66) | <1 0 0> | <0 1 0> | 62.7 |
GdScO3 (mp-5690) | <0 1 0> | <0 1 1> | 88.8 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 1> | 109.2 |
GdScO3 (mp-5690) | <1 0 0> | <0 1 1> | 88.8 |
GdScO3 (mp-5690) | <1 1 0> | <0 1 0> | 62.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 313.7 |
Mg (mp-153) | <0 0 1> | <0 1 0> | 313.7 |
Mg (mp-153) | <1 0 0> | <0 1 0> | 251.0 |
InSb (mp-20012) | <1 1 0> | <1 1 0> | 178.4 |
PbSe (mp-2201) | <1 0 0> | <0 1 0> | 313.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mn3GeC (mp-22706) | 0.4218 | 0.086 | 3 |
CaTiO3 (mp-3442) | 0.4404 | 0.018 | 3 |
Cr3AsN (mp-22209) | 0.4204 | 0.051 | 3 |
BaPbO3 (mp-20991) | 0.4414 | 0.003 | 3 |
SrZrO3 (mp-5076) | 0.4364 | 0.013 | 3 |
Sr2GdRuO6 (mp-1079192) | 0.3398 | 0.558 | 4 |
Sr2YTaO6 (mp-1080719) | 0.3339 | 0.017 | 4 |
Sr2CoWO6 (mp-18771) | 0.3733 | 0.010 | 4 |
Sr2TaInO6 (mp-1086666) | 0.3329 | 0.005 | 4 |
Sr2MnMoO6 (mp-1095141) | 0.3338 | 0.007 | 4 |
SrLaMnWO6 (mp-690608) | 0.4015 | 0.072 | 5 |
Sr4La4Mn7CuO24 (mp-698710) | 0.5320 | 0.121 | 5 |
Sr7PrFe4(MoO6)4 (mp-698609) | 0.4630 | 0.007 | 5 |
Na3LaTi2Nb2O12 (mp-695512) | 0.4583 | 0.017 | 5 |
SrLaMnWO6 (mp-39626) | 0.4048 | 0.072 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Na_pv La Mg_pv W_pv O |
Final Energy/Atom-7.0905 eV |
Corrected Energy-158.9299 eV
Uncorrected energy = -141.8099 eV
Composition-based energy adjustment (-0.687 eV/atom x 12.0 atoms) = -8.2440 eV
Composition-based energy adjustment (-4.438 eV/atom x 2.0 atoms) = -8.8760 eV
Corrected energy = -158.9299 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)