Final Magnetic Moment0.028 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.274 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.00 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.008 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4212 [90] |
HallP 4ab 2ab |
Point Group422 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 284.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 214.6 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 284.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 284.3 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 214.6 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 284.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 286.1 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 143.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 214.6 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 143.0 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 286.1 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 284.3 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 189.5 |
BaTiO3 (mp-5986) | <1 1 1> | <1 1 0> | 202.3 |
NdGaO3 (mp-3196) | <0 1 1> | <1 0 0> | 214.6 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 214.6 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 284.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 189.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 284.3 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 214.6 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 101.1 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 286.1 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 214.6 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 71.5 |
BN (mp-984) | <1 0 0> | <1 0 0> | 286.1 |
Al (mp-134) | <1 1 1> | <0 0 1> | 284.3 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 286.1 |
GdScO3 (mp-5690) | <0 1 1> | <1 0 0> | 214.6 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 284.3 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 286.1 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 214.6 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 214.6 |
C (mp-48) | <1 0 0> | <1 0 0> | 286.1 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 1> | 237.4 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 286.1 |
WSe2 (mp-1821) | <1 0 0> | <1 0 0> | 143.0 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 284.3 |
ZrO2 (mp-2858) | <0 0 1> | <1 0 0> | 214.6 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 284.3 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 189.5 |
YAlO3 (mp-3792) | <1 0 0> | <1 1 0> | 202.3 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 214.6 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 94.8 |
CdWO4 (mp-19387) | <1 0 1> | <1 0 0> | 214.6 |
CdWO4 (mp-19387) | <1 1 1> | <1 1 0> | 101.1 |
TiO2 (mp-390) | <0 0 1> | <0 0 1> | 189.5 |
TiO2 (mp-390) | <1 0 0> | <0 0 1> | 189.5 |
TiO2 (mp-390) | <1 1 0> | <1 0 0> | 214.6 |
MgF2 (mp-1249) | <1 0 1> | <1 0 0> | 286.1 |
ZnO (mp-2133) | <1 0 1> | <1 0 1> | 118.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Ba_sv V_pv Cu_pv P O |
Final Energy/Atom-6.7016 eV |
Corrected Energy-388.6442 eV
Uncorrected energy = -361.8862 eV
Composition-based energy adjustment (-0.687 eV/atom x 34.0 atoms) = -23.3580 eV
Composition-based energy adjustment (-1.700 eV/atom x 2.0 atoms) = -3.4000 eV
Corrected energy = -388.6442 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)