Final Magnetic Moment6.019 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-3.279 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.15 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/mbm [127] |
Hall-P 4 2ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 0 0> | 201.0 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 301.5 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 301.5 |
GaAs (mp-2534) | <1 1 1> | <1 1 0> | 284.3 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 150.8 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 161.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 301.5 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 284.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 161.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 201.0 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 301.5 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 284.3 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 284.3 |
Te2Mo (mp-602) | <1 1 0> | <1 1 0> | 284.3 |
BN (mp-984) | <1 0 0> | <1 1 0> | 284.3 |
BN (mp-984) | <1 1 0> | <1 0 0> | 100.5 |
Al (mp-134) | <1 0 0> | <1 1 0> | 213.2 |
Al (mp-134) | <1 1 0> | <1 0 0> | 201.0 |
TeO2 (mp-2125) | <1 1 0> | <1 1 0> | 284.3 |
TeO2 (mp-2125) | <1 1 1> | <1 0 0> | 100.5 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 161.5 |
C (mp-66) | <1 1 0> | <1 0 0> | 301.5 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 301.5 |
Ni (mp-23) | <1 1 0> | <1 0 0> | 301.5 |
BaTiO3 (mp-5986) | <0 0 1> | <1 1 0> | 142.1 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 301.5 |
MoSe2 (mp-1634) | <0 0 1> | <1 0 0> | 301.5 |
C (mp-48) | <1 1 0> | <1 0 0> | 100.5 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 161.5 |
NaCl (mp-22862) | <1 1 1> | <1 1 0> | 284.3 |
ZrO2 (mp-2858) | <0 1 1> | <1 1 0> | 284.3 |
TiO2 (mp-390) | <1 0 1> | <1 1 0> | 284.3 |
ZnO (mp-2133) | <1 0 0> | <1 0 0> | 301.5 |
SrTiO3 (mp-4651) | <1 0 0> | <1 0 0> | 301.5 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 301.5 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 150.8 |
GaP (mp-2490) | <1 1 0> | <1 0 0> | 301.5 |
TbScO3 (mp-31119) | <0 1 0> | <1 0 0> | 301.5 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 50.3 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 0> | 71.1 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 0> | 301.5 |
NdGaO3 (mp-3196) | <0 1 0> | <1 0 0> | 301.5 |
SiC (mp-11714) | <1 0 0> | <1 0 0> | 251.3 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 201.0 |
Ga2O3 (mp-886) | <1 0 0> | <1 0 0> | 301.5 |
Ga2O3 (mp-886) | <1 1 1> | <1 0 0> | 251.3 |
Si (mp-149) | <1 1 0> | <1 0 0> | 301.5 |
C (mp-48) | <0 0 1> | <1 0 0> | 251.3 |
C (mp-48) | <1 0 0> | <1 0 0> | 251.3 |
WSe2 (mp-1821) | <0 0 1> | <1 0 0> | 301.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ba3Nb5O15 (mp-8846) | 0.2868 | 0.005 | 3 |
K9(WO3)20 (mp-761779) | 0.3651 | 0.000 | 3 |
La2Ti3O9 (mp-758038) | 0.6768 | 0.037 | 3 |
K3Fe5F15 (mp-558744) | 0.3485 | 0.494 | 3 |
Ba3Ta5O15 (mp-15021) | 0.2766 | 0.000 | 3 |
K2CeTa5O15 (mp-21542) | 0.0397 | 0.000 | 4 |
K2CeNb5O15 (mp-21546) | 0.1087 | 0.003 | 4 |
K2LaNb5O15 (mp-559549) | 0.0859 | 0.007 | 4 |
K2CeTa5O15 (mp-562331) | 0.0400 | 0.000 | 4 |
K2CeNb5O15 (mp-562704) | 0.1061 | 0.003 | 4 |
Ba3La7Mn2(Co4O15)2 (mp-694945) | 0.6958 | 0.225 | 5 |
Ba3La9Mg7Nb5O36 (mp-695278) | 0.7329 | 0.112 | 5 |
Na3Sr4La3Ti10O30 (mp-695582) | 0.7212 | 0.012 | 5 |
Ba2La2MgTi3O12 (mp-695403) | 0.6974 | 0.032 | 5 |
Ba3La7Mn(Co3O10)3 (mp-704461) | 0.7073 | 0.147 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Eu Ta_pv O |
Final Energy/Atom-9.1698 eV |
Corrected Energy-442.4188 eV
Uncorrected energy = -421.8088 eV
Composition-based energy adjustment (-0.687 eV/atom x 30.0 atoms) = -20.6100 eV
Corrected energy = -442.4188 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)