Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.387 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.61 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap3.984 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 323.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 267.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 60.1 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 264.9 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 323.6 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 200.3 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 110.9 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 300.3 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 300.3 |
GaN (mp-804) | <1 0 0> | <0 1 1> | 186.0 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 264.9 |
SiO2 (mp-6930) | <1 0 0> | <0 1 1> | 278.9 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 323.6 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 258.9 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 267.0 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 90.1 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 93.0 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 200.3 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 300.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 0> | 264.9 |
LiF (mp-1138) | <1 0 0> | <1 1 0> | 264.9 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 264.9 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 323.6 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 90.1 |
TePb (mp-19717) | <1 1 0> | <1 0 1> | 180.2 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 194.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 323.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 267.0 |
GaSe (mp-1943) | <1 0 0> | <1 1 0> | 264.9 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 278.9 |
BN (mp-984) | <1 0 0> | <1 1 0> | 176.6 |
BN (mp-984) | <1 0 1> | <1 1 0> | 264.9 |
BN (mp-984) | <1 1 0> | <0 1 0> | 64.7 |
BN (mp-984) | <1 1 1> | <1 0 0> | 240.2 |
Al (mp-134) | <1 0 0> | <1 1 0> | 264.9 |
TeO2 (mp-2125) | <1 1 1> | <0 0 1> | 200.3 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 0> | 264.9 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 0> | 240.2 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 323.6 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 240.2 |
Fe3O4 (mp-19306) | <1 1 0> | <0 0 1> | 200.3 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 300.3 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 240.2 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 200.3 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 180.2 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 258.9 |
Al (mp-134) | <1 1 0> | <1 0 0> | 180.2 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 1> | 110.9 |
LiGaO2 (mp-5854) | <0 1 1> | <0 1 0> | 129.4 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 1> | 278.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.87 | 0.00 | 0.03 |
0.00 | 2.76 | -0.00 |
0.03 | -0.00 | 2.88 |
Dielectric Tensor εij (total) |
||
---|---|---|
9.80 | 0.00 | -0.18 |
0.00 | 9.34 | -0.00 |
-0.18 | -0.00 | 6.83 |
Polycrystalline dielectric constant
εpoly∞
2.84
|
Polycrystalline dielectric constant
εpoly
8.66
|
Refractive Index n1.68 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LaAlO3 (mp-771698) | 0.7430 | 0.057 | 3 |
Na2Si3O7 (mp-556198) | 0.7355 | 0.016 | 3 |
K15Mo7N19 (mp-1029869) | 0.7340 | 0.000 | 3 |
K15Re7N19 (mp-1029863) | 0.7093 | 0.000 | 3 |
Na15Cr7N19 (mp-1029705) | 0.7418 | 0.000 | 3 |
Li3Sb5(PO4)6 (mp-26281) | 0.6091 | 0.019 | 4 |
LiSnPO4 (mp-757885) | 0.6446 | 0.078 | 4 |
MgCr2(PO4)2 (mvc-10057) | 0.6499 | 0.048 | 4 |
Li3Bi(PO4)2 (mp-850185) | 0.6030 | 0.101 | 4 |
Na2ZnPHO5 (mp-758238) | 0.7496 | 0.000 | 5 |
KNaLi2(SO4)2 (mp-14484) | 0.7477 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff700 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: K_sv Li_sv V_pv O |
Final Energy/Atom-5.9512 eV |
Corrected Energy-104.1156 eV
Uncorrected energy = -95.2196 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Composition-based energy adjustment (-1.700 eV/atom x 2.0 atoms) = -3.4000 eV
Corrected energy = -104.1156 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)