Final Magnetic Moment0.016 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-3.139 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.97 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.766 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <0 1 0> | 252.9 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 177.5 |
TePb (mp-19717) | <1 0 0> | <0 1 0> | 303.5 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 180.6 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 303.5 |
BN (mp-984) | <0 0 1> | <0 1 0> | 202.3 |
BN (mp-984) | <1 0 0> | <0 1 0> | 252.9 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 303.5 |
SiC (mp-7631) | <0 0 1> | <0 1 0> | 303.5 |
MgO (mp-1265) | <1 0 0> | <0 1 0> | 252.9 |
TiO2 (mp-2657) | <0 0 1> | <0 1 0> | 202.3 |
TiO2 (mp-2657) | <1 0 0> | <0 1 0> | 252.9 |
TiO2 (mp-2657) | <1 1 0> | <0 1 0> | 252.9 |
C (mp-66) | <1 1 0> | <1 0 0> | 180.6 |
LaF3 (mp-905) | <0 0 1> | <1 0 0> | 180.6 |
LaF3 (mp-905) | <1 1 0> | <1 0 0> | 180.6 |
InSb (mp-20012) | <1 0 0> | <0 1 0> | 303.5 |
BaTiO3 (mp-5986) | <1 0 1> | <0 1 0> | 303.5 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 0> | 303.5 |
NdGaO3 (mp-3196) | <1 1 1> | <0 1 0> | 202.3 |
SiC (mp-11714) | <0 0 1> | <0 1 0> | 303.5 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 252.9 |
Au (mp-81) | <1 0 0> | <0 1 0> | 303.5 |
ZrO2 (mp-2858) | <0 0 1> | <0 1 0> | 303.5 |
ZrO2 (mp-2858) | <1 1 -1> | <0 1 0> | 303.5 |
ZrO2 (mp-2858) | <1 1 0> | <0 1 0> | 202.3 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 303.5 |
YAlO3 (mp-3792) | <0 0 1> | <0 1 0> | 303.5 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 0> | 303.5 |
MgF2 (mp-1249) | <0 0 1> | <0 1 0> | 202.3 |
TiO2 (mp-390) | <1 0 1> | <0 1 0> | 151.7 |
MgF2 (mp-1249) | <1 1 1> | <0 1 0> | 151.7 |
Cu (mp-30) | <1 1 0> | <0 1 0> | 252.9 |
LiAlO2 (mp-3427) | <0 0 1> | <0 1 0> | 303.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La5(SiN3)3 (mp-569576) | 0.7231 | 0.000 | 3 |
Ba4Al2O7 (mp-560978) | 0.7151 | 0.000 | 3 |
Ce5(SiN3)3 (mp-571312) | 0.6947 | 0.062 | 3 |
Rb6U5V2O23 (mp-704193) | 0.5569 | 0.001 | 4 |
K6U2Mo4O21 (mp-704736) | 0.7230 | 0.000 | 4 |
Rb6U5V2O23 (mp-581453) | 0.2944 | 0.000 | 4 |
Na6U(SO5)4 (mp-867972) | 0.7195 | 0.146 | 4 |
Rb7U8V2ClO32 (mp-704417) | 0.7434 | 0.003 | 5 |
Ca7NbSi4O17F (mp-542863) | 0.7038 | 0.000 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: K_sv U V_pv O |
Final Energy/Atom-8.0163 eV |
Corrected Energy-616.2071 eV
-616.2071 eV = -577.1738 eV (uncorrected energy) - 32.3053 eV (MP Anion Correction) - 6.7280 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)