Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.272 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.015 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.50 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTeO3 + TeF6 + WO3 |
Band Gap3.056 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CdS (mp-672) | <1 0 1> | <0 1 1> | 130.6 |
TiO2 (mp-2657) | <0 0 1> | <1 1 -1> | 195.8 |
C (mp-66) | <1 0 0> | <1 0 -1> | 153.5 |
Mg (mp-153) | <1 1 1> | <0 0 1> | 207.9 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 221.2 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 221.2 |
BaTiO3 (mp-5986) | <1 1 0> | <0 1 0> | 217.1 |
SiC (mp-11714) | <1 1 1> | <1 0 0> | 110.6 |
C (mp-48) | <1 0 1> | <0 1 1> | 261.3 |
CdWO4 (mp-19387) | <1 0 0> | <1 0 0> | 221.2 |
TiO2 (mp-390) | <1 1 1> | <1 0 0> | 110.6 |
MgF2 (mp-1249) | <1 0 0> | <0 1 1> | 130.6 |
ZnO (mp-2133) | <0 0 1> | <0 1 0> | 217.1 |
ZnO (mp-2133) | <1 0 1> | <0 1 0> | 217.1 |
Al2O3 (mp-1143) | <0 0 1> | <1 0 0> | 221.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V3OF11 (mp-764082) | 0.5846 | 0.016 | 3 |
V3OF11 (mp-779357) | 0.5843 | 0.016 | 3 |
V3OF11 (mp-763267) | 0.5901 | 0.016 | 3 |
V3OF11 (mp-764680) | 0.5857 | 0.078 | 3 |
V3OF11 (mp-781061) | 0.5788 | 0.016 | 3 |
Te4Mo(OF4)5 (mp-578688) | 0.2658 | 0.005 | 4 |
Sb2SeI2F11 (mp-558073) | 0.5684 | 0.000 | 4 |
Sb2SNF11 (mp-560450) | 0.7285 | 0.067 | 4 |
MgAs2(XeF8)2 (mp-556078) | 0.7340 | 0.000 | 4 |
ReTe5O6F25 (mp-649177) | 0.7306 | 0.026 | 4 |
Sb11F43 (mp-28294) | 0.7413 | 0.000 | 2 |
HgSb4C2(OF11)2 (mp-556903) | 0.6873 | 0.080 | 5 |
Sb4OsC6(O3F11)2 (mp-558754) | 0.6257 | 0.084 | 5 |
Sb2OsC4(OF3)4 (mp-559010) | 0.7357 | 0.057 | 5 |
Sb4RuC6(O3F11)2 (mp-555952) | 0.6242 | 0.092 | 5 |
FeSb4C6(O3F11)2 (mp-19590) | 0.6121 | 0.243 | 5 |
Sb4IrC5ClO5F22 (mp-555612) | 0.5140 | 0.108 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesW: 6.2 eV |
PseudopotentialsVASP PAW: Te W_pv O F |
Final Energy/Atom-4.6326 eV |
Corrected Energy-293.6780 eV
-293.6780 eV = -277.9531 eV (uncorrected energy) - 8.7020 eV (MP Advanced Correction) - 7.0229 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)