Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.282 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.078 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCO2 + SbF4 + CF4 + N2 |
Band Gap3.961 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 298.9 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 224.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 224.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 224.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 224.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 298.9 |
BN (mp-984) | <1 0 0> | <1 0 -1> | 173.9 |
BN (mp-984) | <1 1 0> | <0 0 1> | 298.9 |
BN (mp-984) | <1 0 1> | <0 0 1> | 298.9 |
Al (mp-134) | <1 1 1> | <0 0 1> | 224.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 298.9 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 149.4 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 224.1 |
TiO2 (mp-2657) | <1 1 0> | <0 0 1> | 298.9 |
GdScO3 (mp-5690) | <0 1 1> | <0 0 1> | 224.1 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 224.1 |
LaF3 (mp-905) | <1 0 0> | <1 0 0> | 163.1 |
LaF3 (mp-905) | <1 1 0> | <1 0 1> | 184.8 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 298.9 |
TbScO3 (mp-31119) | <1 0 1> | <0 0 1> | 224.1 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 224.1 |
MoSe2 (mp-1634) | <1 0 0> | <0 0 1> | 149.4 |
C (mp-48) | <1 0 0> | <1 0 -1> | 173.9 |
C (mp-48) | <1 0 1> | <0 0 1> | 298.9 |
WSe2 (mp-1821) | <1 0 0> | <0 0 1> | 149.4 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 224.1 |
YAlO3 (mp-3792) | <1 0 0> | <1 0 0> | 163.1 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 224.1 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 163.1 |
CdWO4 (mp-19387) | <1 0 1> | <0 0 1> | 224.1 |
TiO2 (mp-390) | <0 0 1> | <1 0 -1> | 173.9 |
TiO2 (mp-390) | <1 0 0> | <0 0 1> | 74.7 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 224.1 |
LiAlO2 (mp-3427) | <0 0 1> | <1 0 0> | 163.1 |
LiAlO2 (mp-3427) | <1 0 1> | <0 0 1> | 298.9 |
LiAlO2 (mp-3427) | <1 1 1> | <0 0 1> | 224.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SbKr3F11 (mp-30013) | 0.4700 | 0.006 | 3 |
AsXeF7 (mp-27750) | 0.5016 | 0.000 | 3 |
CrXeF6 (mp-558341) | 0.4042 | 0.000 | 3 |
WN3F5 (mp-558743) | 0.5829 | 0.125 | 3 |
AsXe2F9 (mp-637062) | 0.5571 | 0.000 | 3 |
MgAs2(XeF5)4 (mp-555546) | 0.4214 | 0.000 | 4 |
CuSb2(XeF8)2 (mp-606617) | 0.5720 | 0.000 | 4 |
MgAs2(XeF8)2 (mp-556078) | 0.5720 | 0.000 | 4 |
CdP2Xe5F22 (mp-556171) | 0.5450 | 0.000 | 4 |
MnH(CO)4 (mp-745016) | 0.6062 | 0.689 | 4 |
TiF4 (mp-28974) | 0.6637 | 0.000 | 2 |
WN18 (mp-672264) | 0.6495 | 0.285 | 2 |
MnTeC5O6F5 (mp-650943) | 0.5254 | 0.493 | 5 |
HgSb4C2(OF11)2 (mp-556903) | 0.6384 | 0.080 | 5 |
CSNOF5 (mp-672266) | 0.5552 | 0.247 | 5 |
Sb2OsC4(OF3)4 (mp-559010) | 0.5018 | 0.057 | 5 |
FeSb4C6(O3F11)2 (mp-19590) | 0.6280 | 0.242 | 5 |
Sb4IrC5ClO5F22 (mp-555612) | 0.5864 | 0.108 | 6 |
Tl2HPtC5N5O (mp-601902) | 0.7427 | 0.248 | 6 |
ReAsC5SNO5F7 (mp-565400) | 0.6854 | 0.168 | 7 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sb C N O F |
Final Energy/Atom-5.1990 eV |
Corrected Energy-534.1671 eV
Uncorrected energy = -499.1031 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Composition-based energy adjustment (-0.462 eV/atom x 64.0 atoms) = -29.5680 eV
Corrected energy = -534.1671 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)