Final Magnetic Moment5.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.155 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap1.965 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 1 1> | 125.7 |
AlN (mp-661) | <1 0 0> | <1 -1 0> | 156.6 |
AlN (mp-661) | <1 1 0> | <1 -1 -1> | 189.3 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 258.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 235.5 |
GaAs (mp-2534) | <1 1 0> | <1 1 -1> | 235.5 |
GaN (mp-804) | <1 0 0> | <0 1 -1> | 82.8 |
GaN (mp-804) | <1 1 1> | <0 1 0> | 184.9 |
SiO2 (mp-6930) | <0 0 1> | <0 1 -1> | 331.0 |
SiO2 (mp-6930) | <1 0 0> | <1 0 -1> | 194.2 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 184.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 184.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 267.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 267.9 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 -1> | 235.5 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 274.3 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 188.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 -1 0> | 208.8 |
InAs (mp-20305) | <1 0 0> | <0 1 -1> | 331.0 |
InAs (mp-20305) | <1 1 1> | <0 1 -1> | 331.0 |
LaAlO3 (mp-2920) | <1 0 0> | <1 -1 0> | 208.8 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 235.5 |
ZnSe (mp-1190) | <1 1 0> | <1 1 -1> | 235.5 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 282.6 |
AlN (mp-661) | <0 0 1> | <0 1 1> | 125.7 |
AlN (mp-661) | <1 0 1> | <1 -1 -1> | 126.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 267.9 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 295.8 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 282.6 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 -1> | 289.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 47.1 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 235.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 339.9 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 332.8 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 258.9 |
CdS (mp-672) | <1 0 1> | <1 1 -1> | 235.5 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 147.9 |
CdS (mp-672) | <1 1 1> | <1 -1 1> | 265.2 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 114.8 |
GaN (mp-804) | <1 0 1> | <1 -1 0> | 261.0 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 200.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 235.5 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 47.1 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 235.5 |
SiO2 (mp-6930) | <1 0 1> | <1 1 -1> | 176.6 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 266.8 |
KCl (mp-23193) | <1 1 0> | <1 0 -1> | 291.3 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 153.1 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 282.6 |
YVO4 (mp-19133) | <1 0 1> | <1 1 1> | 274.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
4.61 | 0.36 | -0.08 |
0.36 | 5.07 | -0.09 |
-0.08 | -0.09 | 5.24 |
Dielectric Tensor εij (total) |
||
---|---|---|
12.25 | 4.53 | -2.01 |
4.53 | 15.32 | -1.00 |
-2.01 | -1.00 | 19.91 |
Polycrystalline dielectric constant
εpoly∞
4.97
|
Polycrystalline dielectric constant
εpoly
15.83
|
Refractive Index n2.23 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cr2PO5 (mp-770913) | 0.4073 | 0.049 | 3 |
Na2Ge2O5 (mp-780053) | 0.5284 | 0.010 | 3 |
Sn2Ge2O7 (mp-768877) | 0.6208 | 0.039 | 3 |
Ge2MoO6 (mvc-8403) | 0.5895 | 0.087 | 3 |
Cr5(PO4)4 (mp-775246) | 0.6211 | 0.007 | 3 |
Mg3Fe2(Si2O7)2 (mvc-5085) | 0.4608 | 0.099 | 4 |
Zn3Co2(Si2O7)2 (mvc-5029) | 0.4534 | 0.133 | 4 |
NiBiAsO5 (mp-565521) | 0.3352 | 0.000 | 4 |
MnBiAsO5 (mp-565979) | 0.3198 | 0.000 | 4 |
LiFeP2O7 (mp-697764) | 0.4793 | 0.021 | 4 |
Li7MnP4O14F (mp-762708) | 0.6517 | 0.068 | 5 |
Li7FeP4O14F (mp-762690) | 0.6258 | 0.066 | 5 |
KNa2Zn3(PO4)3 (mp-14536) | 0.6987 | 0.001 | 5 |
CuAg7As4ClO14 (mp-653450) | 0.6523 | 0.017 | 5 |
LiCuPO4F (mp-25405) | 0.6430 | 0.045 | 5 |
Run TypeGGA+U |
Energy Cutoff700 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVV: 3.25 eV |
PseudopotentialsVASP PAW: Mn_pv V_pv Bi O |
Final Energy/Atom-7.1549 eV |
Corrected Energy-128.2266 eV
-128.2266 eV = -114.4780 eV (uncorrected energy) - 7.0229 eV (MP Anion Correction) - 6.7257 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)