Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.432 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.004 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.58 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSm2(MoO4)3 + SbO2 + MoO2 |
Band Gap3.218 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/c [15] |
Hall-C 2yc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 241.8 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 192.4 |
C (mp-66) | <1 0 0> | <0 1 0> | 241.8 |
C (mp-66) | <1 1 1> | <0 1 0> | 241.8 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 0> | 241.8 |
WS2 (mp-224) | <1 1 0> | <1 0 0> | 160.3 |
CaCO3 (mp-3953) | <0 0 1> | <0 1 0> | 241.8 |
YAlO3 (mp-3792) | <1 0 0> | <1 0 0> | 160.3 |
CdWO4 (mp-19387) | <0 1 0> | <0 1 0> | 241.8 |
MgF2 (mp-1249) | <1 0 1> | <0 1 0> | 241.8 |
LiAlO2 (mp-3427) | <0 0 1> | <0 1 0> | 241.8 |
Al2O3 (mp-1143) | <1 0 0> | <0 0 1> | 192.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Gd2Mo5O18 (mp-704238) | 0.5186 | 0.008 | 3 |
Y2Cr3O12 (mvc-12912) | 0.6029 | 0.000 | 3 |
U(WO4)2 (mp-704795) | 0.6241 | 0.195 | 3 |
Eu2Mo5O18 (mp-704384) | 0.5249 | 0.310 | 3 |
Ce(WO4)2 (mp-779827) | 0.6347 | 0.110 | 3 |
EuMoClO4 (mp-608717) | 0.6316 | 0.527 | 4 |
YSbMo2O9 (mp-566814) | 0.0848 | 0.034 | 4 |
LaSbMo2O9 (mp-566951) | 0.1239 | 0.000 | 4 |
NdSbMo2O9 (mp-566695) | 0.0545 | 0.000 | 4 |
DySbMo2O9 (mp-566757) | 0.0879 | 0.016 | 4 |
Na2YMoPO8 (mp-567058) | 0.6308 | 0.004 | 5 |
Na2ErMoPO8 (mp-567364) | 0.6164 | 0.003 | 5 |
Na2HoMoPO8 (mp-565656) | 0.6227 | 0.004 | 5 |
Na2DyMoPO8 (mp-566312) | 0.6250 | 0.004 | 5 |
Na2LuMoPO8 (mp-567034) | 0.6137 | 0.003 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMo: 4.38 eV |
PseudopotentialsVASP PAW: Sm_3 Sb Mo_pv O |
Final Energy/Atom-7.1767 eV |
Corrected Energy-426.7212 eV
-426.7212 eV = -373.1908 eV (uncorrected energy) - 28.2480 eV (MP Advanced Correction) - 25.2824 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)