Final Magnetic Moment3.307 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-2.937 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.073 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.40 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTiO2 + Mn |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFd3m [227] |
HallF 4d 2 3 1d |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 149.9 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 299.7 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 106.0 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 74.9 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 106.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 299.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 149.9 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 211.9 |
Ag (mp-124) | <1 0 0> | <1 1 1> | 259.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 224.8 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 299.7 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 211.9 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 211.9 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 299.7 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 74.9 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 106.0 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 129.8 |
C (mp-66) | <1 1 1> | <1 0 0> | 224.8 |
LaF3 (mp-905) | <0 0 1> | <1 0 0> | 224.8 |
PbS (mp-21276) | <1 0 0> | <1 0 0> | 74.9 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 106.0 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 149.9 |
Ni (mp-23) | <1 1 0> | <1 1 0> | 106.0 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 74.9 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 106.0 |
BaTiO3 (mp-5986) | <1 0 1> | <1 1 0> | 211.9 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 299.7 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 211.9 |
Si (mp-149) | <1 0 0> | <1 0 0> | 149.9 |
Au (mp-81) | <1 0 0> | <1 1 1> | 259.6 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 74.9 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 106.0 |
NaCl (mp-22862) | <1 0 0> | <1 0 0> | 299.7 |
CaCO3 (mp-3953) | <0 0 1> | <1 0 0> | 224.8 |
CaCO3 (mp-3953) | <1 1 0> | <1 0 0> | 149.9 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 149.9 |
CsI (mp-614603) | <1 0 0> | <1 0 0> | 299.7 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 74.9 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 106.0 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 149.9 |
SrTiO3 (mp-4651) | <1 1 0> | <1 0 0> | 299.7 |
Cu (mp-30) | <1 1 1> | <1 0 0> | 224.8 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 299.7 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 149.9 |
Fe2O3 (mp-24972) | <0 0 1> | <1 0 0> | 224.8 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 74.9 |
ZnTe (mp-2176) | <1 1 0> | <1 1 0> | 106.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Co2CuO4 (mp-34146) | 0.0035 | 0.029 | 3 |
ZnCr2O4 (mp-19410) | 0.0108 | 0.000 | 3 |
Cr2CoO4 (mp-24868) | 0.0037 | 0.000 | 3 |
ZnCr2O4 (mvc-11550) | 0.0110 | 0.000 | 3 |
Mg(GaO2)2 (mp-4590) | 0.0102 | 0.007 | 3 |
Li2TiFe3O8 (mp-850231) | 0.0682 | 0.045 | 4 |
Li2MnCo3O8 (mp-761737) | 0.0678 | 0.028 | 4 |
Li2Fe3CuO8 (mp-772689) | 0.0588 | 0.046 | 4 |
Li2V3CoO8 (mp-765546) | 0.0570 | 0.223 | 4 |
Li2Ti3CrO8 (mp-771759) | 0.0523 | 0.005 | 4 |
Hf3N4 (mp-755988) | 0.1536 | 0.016 | 2 |
In3S4 (mp-556597) | 0.0799 | 0.042 | 2 |
Co3O4 (mp-18748) | 0.1249 | 0.046 | 2 |
Sn3N4 (mp-16031) | 0.1021 | 0.000 | 2 |
Ge3N4 (mp-476) | 0.1389 | 0.109 | 2 |
Li4Cr2Fe3Co3O16 (mp-775698) | 0.3899 | 0.897 | 5 |
Li14Mn22Cr3Cu3O56 (mp-735790) | 0.3596 | 0.014 | 5 |
Li4Mn3Cr3(CuO8)2 (mp-765456) | 0.3625 | 0.069 | 5 |
Li4Cr3Cu3(SbO8)2 (mp-783908) | 0.3891 | 0.035 | 5 |
Li4Cr3Fe3(SbO8)2 (mp-771925) | 0.3950 | 6.495 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Ti_pv Mn_pv O |
Final Energy/Atom-8.6876 eV |
Corrected Energy-130.4583 eV
Uncorrected energy = -121.6263 eV
Composition-based energy adjustment (-0.687 eV/atom x 8.0 atoms) = -5.4960 eV
Composition-based energy adjustment (-1.668 eV/atom x 2.0 atoms) = -3.3360 eV
Corrected energy = -130.4583 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)