Final Magnetic Moment0.151 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.714 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.99 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToV2Cd2O7 + Sr2V2O7 |
Band Gap3.169 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP41212 [92] |
HallP 4abw 2nw |
Point Group422 |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 257.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 205.7 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 205.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 257.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 205.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 257.2 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 51.4 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 205.7 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 205.7 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 154.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 308.6 |
Al (mp-134) | <1 0 0> | <0 0 1> | 257.2 |
Al (mp-134) | <1 1 1> | <0 0 1> | 257.2 |
LiGaO2 (mp-5854) | <1 0 1> | <0 0 1> | 257.2 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 154.3 |
C (mp-66) | <1 1 0> | <0 0 1> | 257.2 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 257.2 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 154.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 257.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 257.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 257.2 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 257.2 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 257.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 154.3 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 186.2 |
BN (mp-984) | <1 0 0> | <0 0 1> | 154.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 154.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 257.2 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 257.2 |
C (mp-66) | <1 0 0> | <0 0 1> | 51.4 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 308.6 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 154.3 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 154.3 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 308.6 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 308.6 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 257.2 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 205.7 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 257.2 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 205.7 |
BaTiO3 (mp-5986) | <1 1 1> | <0 0 1> | 257.2 |
NdGaO3 (mp-3196) | <0 1 0> | <0 0 1> | 257.2 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 257.2 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 257.2 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 205.7 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 257.2 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 51.4 |
Ge (mp-32) | <1 0 0> | <0 0 1> | 257.2 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 257.2 |
LiAlO2 (mp-3427) | <1 0 1> | <0 0 1> | 257.2 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 257.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ca11Cr7O28 (mp-694886) | 0.6192 | 0.107 | 3 |
LaMoN3 (mp-989631) | 0.6376 | 0.000 | 3 |
SrTcN3 (mp-989627) | 0.6033 | 0.000 | 3 |
LaTcN3 (mp-989619) | 0.6511 | 0.000 | 3 |
LaCrN3 (mp-989612) | 0.5904 | 0.000 | 3 |
K3V3(BiO6)2 (mp-622115) | 0.3926 | 0.000 | 4 |
K3Bi2(AsO4)3 (mp-561369) | 0.4565 | 0.000 | 4 |
Li2Ni(PO3)4 (mp-761553) | 0.5523 | 0.069 | 4 |
K3Bi2(PO4)3 (mp-560420) | 0.5426 | 0.000 | 4 |
Na2VS2O9 (mp-566053) | 0.4229 | 0.002 | 4 |
SrMgCu(PO4)2 (mvc-2684) | 0.5570 | 0.040 | 5 |
SrCaCu(PO4)2 (mvc-2806) | 0.5515 | 0.054 | 5 |
SrCaCo(PO4)2 (mvc-3004) | 0.5581 | 0.027 | 5 |
SrCaNi(PO4)2 (mvc-3009) | 0.5294 | 0.033 | 5 |
SrCaCr(PO4)2 (mvc-3018) | 0.5304 | 0.185 | 5 |
Na2Gd2MgSi4(O6F)2 (mp-557538) | 0.7263 | 0.000 | 6 |
NaLiMn2Fe4(PO4)6 (mp-777193) | 0.6460 | 0.018 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: Sr_sv V_pv Cd O |
Final Energy/Atom-7.0335 eV |
Corrected Energy-685.1861 eV
-685.1861 eV = -618.9458 eV (uncorrected energy) - 39.3282 eV (MP Anion Correction) - 26.9120 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)