Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.714 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.027 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.67 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToY2(MoO4)3 |
Band Gap3.553 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPba2 [32] |
HallP 2 2ab |
Point Groupmm2 |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <0 1 0> | 113.0 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 194.6 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 158.4 |
InAs (mp-20305) | <1 1 1> | <1 1 1> | 194.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 194.6 |
Te2W (mp-22693) | <0 1 0> | <0 1 1> | 158.4 |
SiC (mp-11714) | <1 0 1> | <0 1 0> | 226.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 221.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 221.9 |
Au (mp-81) | <1 1 0> | <0 0 1> | 221.9 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 159.9 |
CdSe (mp-2691) | <1 1 1> | <1 1 1> | 194.6 |
C (mp-48) | <0 0 1> | <1 1 1> | 194.6 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 111.0 |
ZrO2 (mp-2858) | <1 0 0> | <0 1 0> | 113.0 |
Ge(Bi3O5)4 (mp-23352) | <1 0 0> | <0 0 1> | 111.0 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 1> | 194.6 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 221.9 |
YAlO3 (mp-3792) | <0 0 1> | <0 0 1> | 111.0 |
YAlO3 (mp-3792) | <0 1 0> | <0 1 1> | 158.4 |
YAlO3 (mp-3792) | <1 0 0> | <0 1 1> | 158.4 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 111.0 |
SiC (mp-7631) | <1 1 0> | <0 1 1> | 158.4 |
TiO2 (mp-390) | <1 0 1> | <0 1 1> | 158.4 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <0 0 1> | 111.0 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <0 1 1> | 158.4 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <1 1 1> | 194.6 |
MgF2 (mp-1249) | <0 0 1> | <0 0 1> | 111.0 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 159.9 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 0 1> | 221.9 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 221.9 |
KP(HO2)2 (mp-23959) | <1 0 0> | <0 0 1> | 111.0 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 221.9 |
Cu (mp-30) | <1 1 0> | <0 0 1> | 111.0 |
GaTe (mp-542812) | <1 0 0> | <0 0 1> | 221.9 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 111.0 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 111.0 |
InSb (mp-20012) | <1 0 0> | <0 0 1> | 221.9 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 159.9 |
ZnTe (mp-2176) | <1 1 0> | <0 1 1> | 158.4 |
ZnTe (mp-2176) | <1 1 1> | <1 1 1> | 194.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Gd2(WO4)3 (mp-778912) | 0.1004 | 0.641 | 3 |
Gd2(MoO4)3 (mp-650449) | 0.0727 | 0.000 | 3 |
Tb2(WO4)3 (mp-770342) | 0.0913 | 0.043 | 3 |
Gd2(MoO4)3 (mp-554558) | 0.0748 | 0.000 | 3 |
Tb2(MoO4)3 (mp-19534) | 0.0536 | 0.000 | 3 |
LuMoClO4 (mp-567057) | 0.5667 | 0.007 | 4 |
CaZr(PO4)2 (mp-554495) | 0.6854 | 0.000 | 4 |
K3Np(MoO5)2 (mp-616718) | 0.6666 | 0.003 | 4 |
NaY(SiO3)2 (mp-560039) | 0.7227 | 0.007 | 4 |
Sr4Al6WO16 (mp-19259) | 0.6934 | 0.012 | 4 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMo: 4.38 eV |
PseudopotentialsVASP PAW: Y_sv Mo_pv O |
Final Energy/Atom-7.7628 eV |
Corrected Energy-603.9512 eV
-603.9512 eV = -527.8693 eV (uncorrected energy) - 42.3720 eV (MP Advanced Correction) - 33.7099 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)