Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.819 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.003 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.23 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLuPO4 + Na2MoO4 |
Band Gap4.197 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinIbca [73] |
Hall-I 2b 2c |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 164.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 164.5 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 246.8 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 164.5 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 246.8 |
SiC (mp-11714) | <1 0 0> | <0 0 1> | 246.8 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 246.8 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 148.8 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 246.8 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 246.8 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 164.5 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 246.8 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 164.5 |
Au (mp-81) | <1 1 0> | <0 0 1> | 246.8 |
Au (mp-81) | <1 1 1> | <0 0 1> | 246.8 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 246.8 |
NaCl (mp-22862) | <1 1 1> | <0 0 1> | 164.5 |
ZrO2 (mp-2858) | <1 0 -1> | <0 0 1> | 246.8 |
YAlO3 (mp-3792) | <1 1 1> | <0 0 1> | 246.8 |
CdWO4 (mp-19387) | <0 0 1> | <0 0 1> | 246.8 |
CdWO4 (mp-19387) | <1 0 0> | <0 0 1> | 246.8 |
MgF2 (mp-1249) | <1 1 0> | <0 0 1> | 82.3 |
MgF2 (mp-1249) | <1 1 1> | <0 0 1> | 246.8 |
CaF2 (mp-2741) | <1 1 1> | <0 0 1> | 164.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
GdAsO4 (mp-757238) | 0.5306 | 0.049 | 3 |
Y2Cr3O12 (mvc-12164) | 0.4965 | 0.034 | 3 |
NaGaH4 (mp-23918) | 0.4922 | 0.000 | 3 |
U(WO4)2 (mp-704795) | 0.5163 | 0.195 | 3 |
Ce(WO4)2 (mp-779827) | 0.5187 | 0.110 | 3 |
CaU(PO4)2 (mp-9360) | 0.4679 | 0.000 | 4 |
CsPr(MoO4)2 (mp-649915) | 0.5782 | 0.000 | 4 |
Na2V2ZnO7 (mp-640807) | 0.5613 | 0.010 | 4 |
K2Th(MoO4)3 (mp-566934) | 0.5635 | 0.011 | 4 |
KEu(MoO4)2 (mp-566325) | 0.5749 | 0.000 | 4 |
InI2 (mp-29312) | 0.7324 | 0.000 | 2 |
GaCl2 (mp-568848) | 0.7466 | 0.000 | 2 |
Na2YMoPO8 (mp-567058) | 0.1064 | 0.004 | 5 |
Na2ErMoPO8 (mp-567364) | 0.0572 | 0.003 | 5 |
Na2TbMoPO8 (mp-565313) | 0.1693 | 0.004 | 5 |
Na2HoMoPO8 (mp-565656) | 0.0877 | 0.004 | 5 |
Na2DyMoPO8 (mp-566312) | 0.0941 | 0.004 | 5 |
Li2Ca3Be3Si3(O6F)2 (mp-560036) | 0.6905 | 0.000 | 6 |
NaCaBeSi2O6F (mp-560721) | 0.7020 | 0.000 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMo: 4.38 eV |
PseudopotentialsVASP PAW: Na_pv Lu_3 Mo_pv P O |
Final Energy/Atom-6.9601 eV |
Corrected Energy-396.7172 eV
Uncorrected energy = -361.9252 eV
Composition-based energy adjustment (-0.687 eV/atom x 32.0 atoms) = -21.9840 eV
Composition-based energy adjustment (-3.202 eV/atom x 4.0 atoms) = -12.8080 eV
Corrected energy = -396.7172 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)