Final Magnetic Moment0.004 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.666 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.002 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.47 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPbI2 |
Band Gap2.447 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP3m1 [156] |
HallP 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 75.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 75.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 319.9 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 338.7 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 169.4 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 225.8 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 56.5 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 169.4 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 244.6 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 357.5 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 357.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 225.8 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 56.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 131.7 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 94.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 301.1 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 94.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 357.5 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 207.9 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 301.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 75.3 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 376.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 319.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 225.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 225.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 188.2 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 75.3 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 263.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 357.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 244.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 225.8 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 131.7 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 225.8 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 263.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 131.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 169.4 |
BN (mp-984) | <1 0 1> | <0 0 1> | 225.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 75.3 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 319.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 169.4 |
Al (mp-134) | <1 0 0> | <0 0 1> | 131.7 |
Al (mp-134) | <1 1 1> | <0 0 1> | 244.6 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 301.1 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 301.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 75.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 131.7 |
LiGaO2 (mp-5854) | <1 0 1> | <1 1 0> | 180.1 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 301.1 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 169.4 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 319.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2UBr6 (mp-675438) | 0.3147 | 0.001 | 3 |
CaPbI4 (mp-754540) | 0.2547 | 0.001 | 3 |
BiTeCl (mp-28944) | 0.1799 | 0.000 | 3 |
BiTeI (mp-22965) | 0.3134 | 0.000 | 3 |
BiTeBr (mp-33723) | 0.1363 | 0.000 | 3 |
SrLa6OsI12 (mp-567419) | 0.6604 | 0.000 | 4 |
NaLa6OsI12 (mp-569905) | 0.5672 | 0.000 | 4 |
LiTi(SeO)2 (mp-1072633) | 0.6972 | 1.437 | 4 |
LiCaNiF6 (mp-608204) | 0.7398 | 0.011 | 4 |
CrTe2 (mp-685055) | 0.0614 | 0.000 | 2 |
PbI2 (mp-680205) | 0.0610 | 0.003 | 2 |
PbI2 (mp-567199) | 0.0618 | 0.001 | 2 |
PbI2 (mp-567542) | 0.0229 | 0.000 | 2 |
PbI2 (mp-580202) | 0.0552 | 0.001 | 2 |
Explore more synthesis descriptions for materials of composition PbI2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pb_d I |
Final Energy/Atom-2.9200 eV |
Corrected Energy-26.2800 eV
-26.2800 eV = -26.2800 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)