Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.837 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.35 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63mc [186]
Hall
P 6c 2c
Point Group
6mm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 415826 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
PbS (mp-21276) <1 1 1> <0 0 1> 0.002 250.0
Ge (mp-32) <1 0 0> <0 0 1> 0.002 365.4
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.003 76.9
Ge (mp-32) <1 1 1> <0 0 1> 0.008 57.7
MgF2 (mp-1249) <1 0 0> <1 0 1> 0.017 160.4
GaAs (mp-2534) <1 0 0> <0 0 1> 0.020 365.4
AlN (mp-661) <1 0 1> <1 0 1> 0.026 160.4
CdTe (mp-406) <1 0 0> <0 0 1> 0.028 307.7
SiC (mp-11714) <0 0 1> <0 0 1> 0.028 57.7
InSb (mp-20012) <1 0 0> <0 0 1> 0.029 307.7
BN (mp-984) <1 0 1> <1 0 0> 0.030 140.8
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.031 281.6
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.032 153.9
SiC (mp-7631) <0 0 1> <0 0 1> 0.034 57.7
LiAlO2 (mp-3427) <1 0 1> <1 1 1> 0.045 127.8
GaAs (mp-2534) <1 1 1> <0 0 1> 0.046 57.7
AlN (mp-661) <1 0 0> <1 0 0> 0.050 140.8
AlN (mp-661) <1 1 0> <1 1 0> 0.050 243.8
Ni (mp-23) <1 0 0> <1 0 1> 0.050 160.4
LiAlO2 (mp-3427) <1 1 1> <0 0 1> 0.056 269.3
ZrO2 (mp-2858) <1 0 0> <1 1 1> 0.069 255.7
InSb (mp-20012) <1 1 1> <0 0 1> 0.073 76.9
ZrO2 (mp-2858) <1 0 1> <1 1 1> 0.076 127.8
YVO4 (mp-19133) <1 0 0> <1 1 1> 0.081 319.6
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.085 57.7
Fe2O3 (mp-24972) <1 1 0> <1 0 0> 0.089 246.4
LiAlO2 (mp-3427) <1 1 0> <1 0 0> 0.090 140.8
CdTe (mp-406) <1 1 1> <0 0 1> 0.093 76.9
LiF (mp-1138) <1 0 0> <0 0 1> 0.096 134.6
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.101 76.9
YAlO3 (mp-3792) <0 0 1> <1 1 1> 0.102 255.7
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.104 182.9
SiC (mp-7631) <1 1 1> <1 0 0> 0.109 246.4
ZrO2 (mp-2858) <1 1 -1> <1 0 0> 0.113 316.7
MgF2 (mp-1249) <1 0 1> <1 0 1> 0.118 80.2
YAlO3 (mp-3792) <1 0 0> <1 1 0> 0.123 121.9
Mg (mp-153) <1 0 0> <0 0 1> 0.128 250.0
TiO2 (mp-390) <0 0 1> <0 0 1> 0.133 307.7
BaTiO3 (mp-5986) <1 1 1> <1 0 0> 0.133 316.7
BaF2 (mp-1029) <1 1 0> <1 0 1> 0.134 280.7
WS2 (mp-224) <1 1 0> <1 0 0> 0.136 316.7
SiC (mp-8062) <1 1 1> <0 0 1> 0.139 134.6
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.141 250.0
NdGaO3 (mp-3196) <1 0 1> <1 0 1> 0.147 160.4
LaF3 (mp-905) <0 0 1> <0 0 1> 0.149 134.6
DyScO3 (mp-31120) <0 1 1> <1 1 1> 0.161 319.6
Mg (mp-153) <1 0 1> <1 0 0> 0.168 281.6
ZnO (mp-2133) <1 1 1> <1 0 1> 0.169 280.7
ZrO2 (mp-2858) <1 0 -1> <1 0 1> 0.170 320.8
TePb (mp-19717) <1 1 0> <0 0 1> 0.172 307.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
146 77 40 0 0 0
77 146 40 0 0 0
40 40 114 0 0 0
0 0 0 48 0 0
0 0 0 0 48 0
0 0 0 0 0 35
Compliance Tensor Sij (10-12Pa-1)
9.8 -4.7 -1.8 0 0 0
-4.7 9.8 -1.8 0 0 0
-1.8 -1.8 10 0 0 0
0 0 0 20.9 0 0
0 0 0 0 20.9 0
0 0 0 0 0 29
Shear Modulus GV
43 GPa
Bulk Modulus KV
80 GPa
Shear Modulus GR
41 GPa
Bulk Modulus KR
77 GPa
Shear Modulus GVRH
42 GPa
Bulk Modulus KVRH
78 GPa
Elastic Anisotropy
0.22
Poisson's Ratio
0.27

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TbSnAu (mp-31413) 0.0355 0.000 3
DySnAu (mp-31414) 0.0620 0.000 3
HoSnAu (mp-568814) 0.0779 0.038 3
TmCuPb (mp-20663) 0.0957 0.000 3
YbBiAu (mp-1077471) 0.0908 0.000 3
EuTl2 (mp-30630) 0.4016 0.000 2
MgGa2 (mp-30651) 0.4540 0.005 2
EuIn2 (mp-636316) 0.3999 0.000 2
YbIn2 (mp-568058) 0.3995 0.000 2
CaIn2 (mp-21068) 0.3930 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Y_sv Sn_d Au
Final Energy/Atom
-5.4141 eV
Corrected Energy
-32.4846 eV
Uncorrected energy = -32.4846 eV Corrected energy = -32.4846 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 415826
Submitted by
User remarks:
  • Yttrium gold stannide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)