Final Magnetic Moment0.908 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.457 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.332 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.22 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCO2 + H8NF5 + GdF3 + CF4 + C |
Band Gap1.306 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP1 [2] |
Hall-P 1 |
Point Group1 |
Crystal Systemtriclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 211.4 |
TeO2 (mp-2125) | <0 1 1> | <1 -1 -1> | 156.8 |
TeO2 (mp-2125) | <1 0 1> | <1 -1 -1> | 156.8 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 238.4 |
Mg (mp-153) | <1 0 1> | <0 0 1> | 267.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 267.3 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 267.3 |
GaP (mp-2490) | <1 1 0> | <1 1 -1> | 174.8 |
BN (mp-984) | <0 0 1> | <1 1 -1> | 174.8 |
BN (mp-984) | <1 0 0> | <0 0 1> | 267.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 267.3 |
TbScO3 (mp-31119) | <0 1 1> | <0 0 1> | 267.3 |
BaTiO3 (mp-5986) | <1 1 0> | <0 0 1> | 267.3 |
C (mp-48) | <1 1 0> | <0 0 1> | 267.3 |
C (mp-48) | <1 1 1> | <1 0 0> | 238.4 |
ZrO2 (mp-2858) | <1 1 1> | <1 0 -1> | 256.1 |
Si (mp-149) | <1 1 0> | <0 1 0> | 211.4 |
C (mp-48) | <1 0 0> | <0 1 0> | 211.4 |
ZrO2 (mp-2858) | <0 1 0> | <1 0 -1> | 256.1 |
MgF2 (mp-1249) | <0 0 1> | <1 0 0> | 238.4 |
MgF2 (mp-1249) | <1 0 1> | <1 -1 -1> | 156.8 |
ZnO (mp-2133) | <0 0 1> | <1 -1 0> | 252.5 |
SiC (mp-8062) | <1 0 0> | <0 1 0> | 211.4 |
CdWO4 (mp-19387) | <1 1 0> | <1 0 1> | 167.1 |
TiO2 (mp-390) | <1 1 0> | <0 0 1> | 267.3 |
CsI (mp-614603) | <1 1 0> | <1 1 -1> | 174.8 |
SrTiO3 (mp-4651) | <1 0 0> | <1 1 -1> | 174.8 |
Cu (mp-30) | <1 1 0> | <1 0 0> | 238.4 |
CaF2 (mp-2741) | <1 1 0> | <1 1 -1> | 174.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
PH8N4Cl (mp-781992) | 0.6471 | 0.006 | 4 |
LaP3(HO)6 (mp-740930) | 0.6279 | 0.154 | 4 |
PH8IN4 (mp-643158) | 0.7245 | 0.000 | 4 |
P2H12N7Cl (mp-758356) | 0.6729 | 0.010 | 4 |
HgC2O2F3 (mp-558982) | 0.7190 | 0.127 | 4 |
InH8C4NO10 (mp-557319) | 0.6253 | 0.028 | 5 |
TiH8C4NO10 (mp-557562) | 0.6201 | 0.078 | 5 |
TiH8C4NO10 (mp-557853) | 0.6264 | 0.078 | 5 |
UH12C4N4O11 (mp-558003) | 0.6729 | 0.495 | 5 |
ZrH36C16(NO4)4 (mp-600208) | 0.6966 | 0.133 | 5 |
DyH6C6Cl3(O3F2)3 (mp-605302) | 0.7487 | 0.192 | 6 |
CaRe2H6C(NO5)2 (mp-696020) | 0.7292 | 0.031 | 6 |
KDyH2C2SO9 (mp-605166) | 0.7491 | 0.025 | 6 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Gd H C N O F |
Final Energy/Atom-6.2377 eV |
Corrected Energy-510.2500 eV
-510.2500 eV = -499.0133 eV (uncorrected energy) - 11.2366 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)