Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.317 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.40 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
3.277 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Imm2 [44]
Hall
I 2 2
Point Group
mm2
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 391265 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Au (mp-81) <1 0 0> <1 1 0> 0.014 86.9
CdWO4 (mp-19387) <0 1 0> <0 0 1> 0.016 345.7
MgF2 (mp-1249) <1 0 0> <1 1 0> 0.020 86.9
TiO2 (mp-2657) <0 0 1> <1 1 0> 0.022 86.9
Ag (mp-124) <1 0 0> <1 1 0> 0.022 86.9
SiC (mp-8062) <1 0 0> <1 1 0> 0.041 173.7
WS2 (mp-224) <1 0 1> <0 0 1> 0.044 230.4
TePb (mp-19717) <1 0 0> <1 1 0> 0.050 86.9
SrTiO3 (mp-4651) <1 0 1> <0 1 0> 0.066 271.6
Ag (mp-124) <1 1 0> <0 0 1> 0.067 268.9
ZrO2 (mp-2858) <1 1 0> <0 1 0> 0.074 316.9
SrTiO3 (mp-4651) <1 0 0> <1 0 0> 0.080 222.4
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.085 192.0
BaTiO3 (mp-5986) <1 0 0> <0 0 1> 0.096 268.9
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.099 192.0
Au (mp-81) <1 1 0> <0 0 1> 0.104 268.9
GaN (mp-804) <1 0 0> <0 0 1> 0.108 153.6
CdTe (mp-406) <1 0 0> <1 1 0> 0.108 86.9
C (mp-48) <1 0 1> <1 0 0> 0.119 296.5
AlN (mp-661) <1 1 1> <0 1 0> 0.126 316.9
InSb (mp-20012) <1 0 0> <1 1 0> 0.130 86.9
MgF2 (mp-1249) <1 0 1> <1 1 0> 0.133 260.6
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.138 192.0
GdScO3 (mp-5690) <1 0 0> <0 0 1> 0.141 230.4
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.143 192.0
MgO (mp-1265) <1 1 1> <1 0 1> 0.159 250.5
MgF2 (mp-1249) <0 0 1> <1 1 0> 0.160 86.9
Al2O3 (mp-1143) <1 0 0> <0 0 1> 0.161 192.0
NaCl (mp-22862) <1 1 1> <1 0 0> 0.191 222.4
NaCl (mp-22862) <1 0 0> <0 0 1> 0.206 192.0
YAlO3 (mp-3792) <0 1 0> <0 1 0> 0.209 316.9
NdGaO3 (mp-3196) <1 0 0> <1 0 0> 0.232 222.4
TbScO3 (mp-31119) <0 0 1> <1 0 0> 0.236 222.4
BN (mp-984) <0 0 1> <0 1 1> 0.237 296.8
Cu (mp-30) <1 1 0> <0 1 1> 0.237 296.8
Te2Mo (mp-602) <1 1 0> <0 0 1> 0.254 192.0
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.254 192.0
SiC (mp-11714) <1 0 1> <0 0 1> 0.258 192.0
Te2W (mp-22693) <0 0 1> <0 0 1> 0.264 153.6
TiO2 (mp-2657) <1 0 1> <1 1 0> 0.265 260.6
Te2W (mp-22693) <1 0 0> <0 0 1> 0.271 192.0
GdScO3 (mp-5690) <0 0 1> <1 0 0> 0.274 222.4
AlN (mp-661) <0 0 1> <1 0 0> 0.278 296.5
Fe3O4 (mp-19306) <1 0 0> <0 1 1> 0.279 296.8
GdScO3 (mp-5690) <0 1 0> <1 0 0> 0.284 222.4
GaN (mp-804) <1 1 0> <0 1 0> 0.294 316.9
SiC (mp-7631) <1 0 0> <0 0 1> 0.294 192.0
MoS2 (mp-1434) <0 0 1> <0 1 1> 0.310 237.5
WS2 (mp-224) <0 0 1> <0 1 1> 0.310 237.5
DyScO3 (mp-31120) <0 0 1> <1 0 0> 0.311 222.4
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
252 91 59 0 0 0
91 296 70 0 0 0
59 70 349 0 0 0
0 0 0 77 0 0
0 0 0 0 117 0
0 0 0 0 0 85
Compliance Tensor Sij (10-12Pa-1)
4.5 -1.3 -0.5 0 0 0
-1.3 3.9 -0.6 0 0 0
-0.5 -0.6 3.1 0 0 0
0 0 0 13 0 0
0 0 0 0 8.5 0
0 0 0 0 0 11.7
Shear Modulus GV
101 GPa
Bulk Modulus KV
148 GPa
Shear Modulus GR
97 GPa
Bulk Modulus KR
147 GPa
Shear Modulus GVRH
99 GPa
Bulk Modulus KVRH
148 GPa
Elastic Anisotropy
0.24
Poisson's Ratio
0.23

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.00000 0.59635 0.00000
0.00000 0.00000 0.00000 -0.21518 0.00000 0.00000
0.97704 -0.21313 0.88615 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
1.33615 C/m2
Crystallographic Direction vmax
-0.00000
-1.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
4.50 0.00 -0.00
0.00 4.59 0.00
-0.00 0.00 4.75
Dielectric Tensor εij (total)
14.51 0.00 0.00
0.00 12.40 0.00
0.00 0.00 13.40
Polycrystalline dielectric constant εpoly
(electronic contribution)
4.61
Polycrystalline dielectric constant εpoly
(total)
13.43
Refractive Index n
2.15
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
BaAl4O7 (mp-1019532) 0.6098 0.024 3
Ge2N2O (mp-859876) 0.6737 0.046 3
Ge2N2O (mp-777483) 0.6973 0.069 3
Ge2N2O (mp-778194) 0.6811 0.035 3
Ba(Si3N4)2 (mp-567771) 0.1814 0.000 3
LiFeSiO4 (mp-851283) 0.7292 0.068 4
Li2FeSi3O8 (mp-767149) 0.7123 0.075 4
Li2Si3NiO8 (mp-863897) 0.6918 0.093 4
LiCoSiO4 (mp-763260) 0.7099 0.241 4
LiCoSiO4 (mp-765142) 0.6642 0.260 4
C2N3 (mp-1078791) 0.6676 0.567 2
LaAl2Si5N9O (mp-677482) 0.5453 0.151 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sr_sv Si N
Final Energy/Atom
-7.8399 eV
Corrected Energy
-117.5984 eV
-117.5984 eV = -117.5984 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 391265
Submitted by
User remarks:
  • Strontium octanitrido hexasilicate

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)