Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.483 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.73 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 66.0 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 110.0 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 153.9 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 1> | 218.6 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 153.9 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 144.4 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 57.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 329.9 |
BaF2 (mp-1029) | <1 1 0> | <0 1 1> | 108.3 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 143.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 197.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 110.0 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 87.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 285.9 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 171.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 88.0 |
GaN (mp-804) | <1 1 1> | <1 0 1> | 87.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 1> | 131.1 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 209.0 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 151.1 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 110.0 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 108.3 |
GaN (mp-804) | <1 0 1> | <1 1 1> | 209.0 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 87.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 1> | 43.7 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 1> | 144.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 285.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 1> | 131.1 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 171.8 |
SiO2 (mp-6930) | <1 1 0> | <0 1 1> | 144.4 |
KCl (mp-23193) | <1 0 0> | <0 1 1> | 324.9 |
KCl (mp-23193) | <1 1 0> | <0 1 1> | 288.8 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 209.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 1> | 131.1 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 57.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 0> | 151.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 218.6 |
InAs (mp-20305) | <1 0 0> | <1 1 0> | 189.6 |
InAs (mp-20305) | <1 1 0> | <0 1 1> | 108.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 66.0 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 114.5 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 144.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 66.0 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 72.2 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 340.0 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 142.2 |
CdS (mp-672) | <1 0 1> | <0 1 0> | 229.0 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 151.1 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 151.1 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 331.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
125 | 62 | 89 | 0 | 0 | 0 |
62 | 110 | 81 | 0 | 0 | 0 |
89 | 81 | 120 | 0 | 0 | 0 |
0 | 0 | 0 | 29 | 0 | 0 |
0 | 0 | 0 | 0 | 37 | 0 |
0 | 0 | 0 | 0 | 0 | 32 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
16.9 | -0.6 | -12.2 | 0 | 0 | 0 |
-0.6 | 18.2 | -12 | 0 | 0 | 0 |
-12.2 | -12 | 25.5 | 0 | 0 | 0 |
0 | 0 | 0 | 34 | 0 | 0 |
0 | 0 | 0 | 0 | 26.9 | 0 |
0 | 0 | 0 | 0 | 0 | 31.3 |
Shear Modulus GV28 GPa |
Bulk Modulus KV91 GPa |
Shear Modulus GR24 GPa |
Bulk Modulus KR89 GPa |
Shear Modulus GVRH26 GPa |
Bulk Modulus KVRH90 GPa |
Elastic Anisotropy0.77 |
Poisson's Ratio0.37 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hf2NiP (mp-5918) | 0.6163 | 0.000 | 3 |
Zr2CoP (mp-29152) | 0.5668 | 0.000 | 3 |
Zr2NiP (mp-29153) | 0.6011 | 0.000 | 3 |
Hf2CoP (mp-29154) | 0.5602 | 0.000 | 3 |
Ba2PtAu (mp-675690) | 0.2311 | 0.003 | 3 |
SrCa2In2Ge (mp-619206) | 0.5111 | 0.106 | 4 |
TmNi (mp-11525) | 0.0973 | 0.000 | 2 |
LuNi (mp-1078899) | 0.1084 | 0.000 | 2 |
YNi (mp-1364) | 0.0835 | 0.000 | 2 |
HoNi (mp-11871) | 0.1029 | 0.000 | 2 |
DyNi (mp-2738) | 0.1132 | 0.000 | 2 |
Si (mp-1001113) | 0.7011 | 0.488 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Er_3 Ni_pv |
Final Energy/Atom-5.6562 eV |
Corrected Energy-45.2499 eV
-45.2499 eV = -45.2499 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)