Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.095 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.103 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToBi4Te3 + Bi2Te3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
TePb (mp-19717) | <1 0 0> | <1 0 0> | 42.3 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 73.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 220.0 |
BN (mp-984) | <0 0 1> | <1 0 0> | 211.7 |
BN (mp-984) | <1 0 1> | <1 1 1> | 220.0 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 211.7 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 1> | 293.3 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 211.7 |
Al (mp-134) | <1 0 0> | <1 0 0> | 211.7 |
Al (mp-134) | <1 1 0> | <1 1 0> | 179.6 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 169.3 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 0> | 179.6 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 239.5 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 42.3 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 59.9 |
CdTe (mp-406) | <1 1 1> | <1 1 1> | 73.3 |
SiC (mp-7631) | <0 0 1> | <1 1 0> | 299.4 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 239.5 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 211.7 |
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 127.0 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 299.4 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 119.7 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 179.6 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 239.5 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 169.3 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 239.5 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 220.0 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 42.3 |
TiO2 (mp-2657) | <1 0 0> | <1 1 1> | 220.0 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 296.4 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 169.3 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 296.4 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 119.7 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 220.0 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 169.3 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 179.6 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 220.0 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 338.7 |
C (mp-66) | <1 0 0> | <1 0 0> | 169.3 |
C (mp-66) | <1 1 0> | <1 0 0> | 338.7 |
C (mp-66) | <1 1 1> | <1 1 1> | 293.3 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 179.6 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 296.4 |
GdScO3 (mp-5690) | <0 1 0> | <1 1 0> | 179.6 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 0> | 179.6 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 338.7 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 211.7 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 299.4 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 42.3 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 59.9 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
71 | 34 | 34 | 0 | 0 | 0 |
34 | 71 | 34 | 0 | 0 | 0 |
34 | 34 | 71 | 0 | 0 | 0 |
0 | 0 | 0 | -6 | 0 | 0 |
0 | 0 | 0 | 0 | -6 | 0 |
0 | 0 | 0 | 0 | 0 | -6 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
20.4 | -6.6 | -6.6 | 0 | 0 | 0 |
-6.6 | 20.4 | -6.6 | 0 | 0 | 0 |
-6.6 | -6.6 | 20.4 | 0 | 0 | 0 |
0 | 0 | 0 | -155.7 | 0 | 0 |
0 | 0 | 0 | 0 | -155.7 | 0 |
0 | 0 | 0 | 0 | 0 | -155.7 |
Shear Modulus GV4 GPa |
Bulk Modulus KV46 GPa |
Shear Modulus GR-14 GPa |
Bulk Modulus KR46 GPa |
Shear Modulus GVRH-5 GPa |
Bulk Modulus KVRH46 GPa |
Elastic Anisotropy-6.28 |
Poisson's Ratio0.56 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sr4SO3 (mp-1079788) | 0.0000 | 0.200 | 3 |
BaSr3O4 (mp-984729) | 0.0000 | 0.044 | 3 |
ScH4Pd3 (mp-981386) | 0.0000 | 0.037 | 3 |
Sr3CdO4 (mp-981103) | 0.0000 | 0.019 | 3 |
SrCa3O4 (mp-978844) | 0.0000 | 0.040 | 3 |
LuBi (mp-568059) | 0.0000 | 0.000 | 2 |
GdTe (mp-574283) | 0.0000 | 0.000 | 2 |
CsBr (mp-571222) | 0.0000 | 0.000 | 2 |
MnO (mp-578625) | 0.0000 | 0.000 | 2 |
PuAs (mp-1000774) | 0.0000 | 0.000 | 2 |
As (mp-10) | 0.0000 | 0.112 | 1 |
Sc (mp-1008681) | 0.0000 | 0.719 | 1 |
Ca (mp-10683) | 0.0000 | 0.400 | 1 |
C (mp-998866) | 0.0000 | 2.755 | 1 |
Sb (mp-133) | 0.0000 | 0.051 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Bi Te |
Final Energy/Atom-3.6113 eV |
Corrected Energy-7.2227 eV
-7.2227 eV = -7.2227 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)