Final Magnetic Moment0.058 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.668 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.12 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.413 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63mc [186] |
HallP 6c 2c |
Point Group6mm |
Crystal Systemhexagonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 75.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 75.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 340.2 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 56.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 170.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 245.7 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 359.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 321.3 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 359.1 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 359.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 226.8 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 321.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 226.8 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 226.8 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 189.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 359.1 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 226.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 94.5 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 245.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 132.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 94.5 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 245.7 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 378.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 56.7 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 132.3 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 132.3 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 226.8 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 264.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 75.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 132.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 359.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 226.8 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 170.1 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 302.4 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 302.4 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 75.6 |
BN (mp-984) | <1 0 1> | <0 0 1> | 226.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 170.1 |
LiNbO3 (mp-3731) | <1 0 1> | <0 0 1> | 321.3 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 94.5 |
Al (mp-134) | <1 1 0> | <0 0 1> | 94.5 |
Al (mp-134) | <1 1 1> | <0 0 1> | 245.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 170.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 132.3 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 302.4 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 75.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 132.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 170.1 |
Al (mp-134) | <1 0 0> | <0 0 1> | 132.3 |
TeO2 (mp-2125) | <1 1 0> | <0 0 1> | 302.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.01085 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.01085 | 0.00000 | 0.00000 |
0.00130 | 0.00130 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.01085 C/m2 |
Crystallographic Direction vmax |
---|
0.00000 |
-1.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
6.04 | -0.00 | 0.00 |
-0.00 | 6.04 | 0.00 |
0.00 | 0.00 | 4.05 |
Dielectric Tensor εij (total) |
||
---|---|---|
24.18 | -0.00 | -0.00 |
-0.00 | 24.18 | -0.00 |
-0.00 | -0.00 | 4.71 |
Polycrystalline dielectric constant
εpoly∞
5.38
|
Polycrystalline dielectric constant
εpoly
17.69
|
Refractive Index n2.32 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2UBr6 (mp-675438) | 0.3174 | 0.001 | 3 |
CaPbI4 (mp-754540) | 0.2458 | 0.001 | 3 |
BiTeCl (mp-28944) | 0.1870 | 0.000 | 3 |
CaPbI4 (mp-753670) | 0.3179 | 0.000 | 3 |
BiTeBr (mp-33723) | 0.1381 | 0.000 | 3 |
SrLa6OsI12 (mp-567419) | 0.6589 | 0.000 | 4 |
NaLa6OsI12 (mp-569905) | 0.5691 | 0.000 | 4 |
LiCaNiF6 (mp-559584) | 0.7468 | 0.011 | 4 |
LiTi(SeO)2 (mp-1072633) | 0.6948 | 1.437 | 4 |
LiCaNiF6 (mp-608204) | 0.7330 | 0.011 | 4 |
CrTe2 (mp-685055) | 0.0666 | 0.000 | 2 |
PbI2 (mp-680205) | 0.0576 | 0.003 | 2 |
PbI2 (mp-567178) | 0.0229 | 0.002 | 2 |
PbI2 (mp-567199) | 0.0682 | 0.001 | 2 |
PbI2 (mp-580202) | 0.0614 | 0.001 | 2 |
Explore more synthesis descriptions for materials of composition PbI2.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff700 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pb_d I |
Final Energy/Atom-2.9220 eV |
Corrected Energy-35.0637 eV
-35.0637 eV = -35.0637 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)