Final Magnetic Moment0.010 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.471 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.042 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.86 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToInSe + In2Se3 |
Band Gap0.502 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 318.2 |
AlN (mp-661) | <1 0 0> | <1 1 -1> | 187.1 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 272.6 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 357.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 238.6 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 223.6 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 298.1 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 238.6 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 298.1 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 318.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 198.9 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 318.2 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 193.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 159.1 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 278.4 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 238.6 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 298.1 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 238.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 278.4 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 90.9 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 149.1 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 119.3 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 223.6 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 298.1 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 198.9 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 238.6 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 119.3 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 119.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 278.4 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 278.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 357.9 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 119.3 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 74.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 318.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 318.2 |
BN (mp-984) | <0 0 1> | <1 0 1> | 272.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 318.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 357.9 |
BN (mp-984) | <1 1 1> | <0 0 1> | 238.6 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 1> | 90.9 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 278.4 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 318.2 |
Al (mp-134) | <1 1 0> | <0 0 1> | 119.3 |
Al (mp-134) | <1 1 1> | <0 0 1> | 278.4 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 -1> | 310.2 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 298.1 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 -1> | 310.2 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 278.4 |
Al (mp-134) | <1 0 0> | <1 0 0> | 149.1 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 298.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaCr2O4 (mvc-11984) | 0.5406 | 0.182 | 3 |
TlIn5Se7 (mp-574279) | 0.1156 | 0.020 | 3 |
TlIn5S7 (mp-562480) | 0.2562 | 0.000 | 3 |
NaFe3O5 (mp-541405) | 0.4957 | 0.699 | 3 |
Mn(SbS2)2 (mp-10412) | 0.5117 | 0.013 | 3 |
Li4TiCo5O12 (mp-771514) | 0.5490 | 0.143 | 4 |
Li4CrCo5O12 (mp-771505) | 0.5588 | 0.150 | 4 |
Li4V5SnO12 (mp-777449) | 0.5662 | 0.115 | 4 |
Li2Co(NiO3)2 (mp-761662) | 0.5337 | 0.073 | 4 |
Li4FeCo5O12 (mp-771206) | 0.5606 | 0.059 | 4 |
In6S7 (mp-555853) | 0.2320 | 0.008 | 2 |
Li4Ti3Mn4(CoO9)2 (mp-775615) | 0.6918 | 0.135 | 5 |
Li4Ti2Mn3(Fe2O9)2 (mp-769444) | 0.5950 | 0.080 | 5 |
Li4Ti2V3Cr4O18 (mp-775447) | 0.6547 | 0.084 | 5 |
Li4TiV4Cr4O18 (mp-767927) | 0.6957 | 0.085 | 5 |
Li4Ti2Fe4(CoO6)3 (mp-776197) | 0.6776 | 0.217 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: In_d Se |
Final Energy/Atom-3.6235 eV |
Corrected Energy-100.8198 eV
Uncorrected energy = -94.2118 eV
Composition-based energy adjustment (-0.472 eV/atom x 14.0 atoms) = -6.6080 eV
Corrected energy = -100.8198 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)