material

CsPbBr3

ID:

mp-567681

DOI:

10.17188/1273990


Tags: Cesium lead bromide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.316 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.78 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
2.892 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 28312 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BaTiO3 (mp-5986) <1 0 0> <0 1 1> 0.003 185.8
SiO2 (mp-6930) <1 0 1> <0 0 1> 0.003 140.5
AlN (mp-661) <1 1 0> <0 0 1> 0.006 327.8
CdTe (mp-406) <1 1 0> <0 1 1> 0.007 185.8
MgF2 (mp-1249) <1 1 0> <0 1 1> 0.007 185.8
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.008 172.7
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.008 172.7
InSb (mp-20012) <1 1 0> <0 1 1> 0.010 185.8
ZnO (mp-2133) <1 1 1> <1 1 0> 0.010 190.4
TiO2 (mp-2657) <1 1 0> <1 1 1> 0.011 196.1
CdWO4 (mp-19387) <0 1 1> <0 0 1> 0.012 281.0
Ni (mp-23) <1 0 0> <1 1 1> 0.012 196.1
SiC (mp-11714) <1 0 0> <0 0 1> 0.013 93.7
LiF (mp-1138) <1 1 1> <1 0 0> 0.013 172.7
AlN (mp-661) <1 0 1> <0 1 0> 0.015 160.4
CaCO3 (mp-3953) <1 0 0> <1 0 0> 0.017 172.7
Ag (mp-124) <1 0 0> <0 0 1> 0.017 327.8
BN (mp-984) <1 0 0> <0 0 1> 0.022 234.2
Ni (mp-23) <1 1 0> <0 0 1> 0.022 140.5
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.022 281.0
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.023 190.4
Au (mp-81) <1 0 0> <0 0 1> 0.024 327.8
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.025 190.4
TiO2 (mp-2657) <1 0 1> <0 0 1> 0.031 234.2
SiO2 (mp-6930) <1 1 0> <1 1 0> 0.032 190.4
MgO (mp-1265) <1 1 0> <0 1 1> 0.032 278.7
MgF2 (mp-1249) <1 0 0> <0 1 0> 0.034 160.4
Ag (mp-124) <1 1 1> <1 0 1> 0.038 178.9
TiO2 (mp-390) <0 0 1> <0 0 1> 0.038 234.2
SiO2 (mp-6930) <0 0 1> <1 0 0> 0.039 172.7
TeO2 (mp-2125) <0 0 1> <1 1 0> 0.041 190.4
BaTiO3 (mp-5986) <1 1 1> <1 0 0> 0.041 172.7
DyScO3 (mp-31120) <0 0 1> <1 1 0> 0.045 190.4
LiGaO2 (mp-5854) <0 1 0> <0 0 1> 0.046 327.8
Au (mp-81) <1 1 1> <1 0 1> 0.047 178.9
TePb (mp-19717) <1 1 0> <0 1 1> 0.048 185.8
TiO2 (mp-2657) <1 0 0> <0 0 1> 0.049 140.5
SiO2 (mp-6930) <1 0 0> <0 0 1> 0.049 327.8
AlN (mp-661) <0 0 1> <0 0 1> 0.051 327.8
SiC (mp-11714) <1 1 0> <0 0 1> 0.059 327.8
Cu (mp-30) <1 1 0> <0 0 1> 0.060 327.8
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.065 234.2
LiGaO2 (mp-5854) <0 0 1> <0 0 1> 0.065 327.8
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.067 172.7
C (mp-66) <1 1 1> <1 0 1> 0.070 178.9
ZnO (mp-2133) <1 0 0> <0 1 0> 0.073 240.6
SiC (mp-7631) <0 0 1> <0 0 1> 0.079 327.8
SiC (mp-11714) <0 0 1> <0 0 1> 0.082 327.8
Fe2O3 (mp-24972) <1 0 0> <0 0 1> 0.090 140.5
C (mp-66) <1 0 0> <0 0 1> 0.092 327.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
16 10 9 0 0 0
10 25 8 0 0 0
9 8 26 0 0 0
0 0 0 6 0 0
0 0 0 0 8 0
0 0 0 0 0 5
Compliance Tensor Sij (10-12Pa-1)
95.8 -29.1 -24.7 0 0 0
-29.1 52.7 -5.7 0 0 0
-24.7 -5.7 49.1 0 0 0
0 0 0 176.5 0 0
0 0 0 0 123.6 0
0 0 0 0 0 194.1
Shear Modulus GV
6 GPa
Bulk Modulus KV
13 GPa
Shear Modulus GR
6 GPa
Bulk Modulus KR
13 GPa
Shear Modulus GVRH
6 GPa
Bulk Modulus KVRH
13 GPa
Elastic Anisotropy
0.45
Poisson's Ratio
0.29

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CsSnI3 (mp-27381) 0.2496 0.003 3
Cs3ClO (mp-562420) 0.3402 0.001 3
CsPbI3 (mp-540839) 0.2848 0.000 3
PrCrSe3 (mp-861512) 0.3295 0.000 3
NdCrSe3 (mp-864797) 0.3423 0.000 3
LaCrS2O (mp-18885) 0.7283 0.023 4
KTh(SbSe3)2 (mp-568904) 0.5944 0.000 4
BaLa(BiS3)2 (mp-555699) 0.6437 0.000 4
BaMgBiF7 (mvc-10353) 0.6775 0.042 4
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cs_sv Pb_d Br
Final Energy/Atom
-3.2203 eV
Corrected Energy
-64.4052 eV
-64.4052 eV = -64.4052 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 28312
Submitted by
User remarks:
  • Cesium lead bromide