material

SrBr2

ID:

mp-567744

DOI:

10.17188/1274023


Tags: Strontium bromide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.505 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.76 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
4.470 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pnma [62]
Hall
-P 2ac 2n
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 15972 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
C (mp-48) <1 1 1> <0 0 1> 0.000 303.7
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.002 189.8
GaN (mp-804) <0 0 1> <0 1 1> 0.006 134.2
SrTiO3 (mp-4651) <1 0 1> <0 1 1> 0.006 268.5
Al2O3 (mp-1143) <1 0 0> <0 0 1> 0.008 189.8
Al2O3 (mp-1143) <1 0 1> <0 0 1> 0.011 265.7
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.011 189.8
GaN (mp-804) <1 0 0> <0 0 1> 0.013 151.8
NdGaO3 (mp-3196) <1 0 1> <0 1 1> 0.015 268.5
Al2O3 (mp-1143) <0 0 1> <0 1 1> 0.016 201.3
Mg (mp-153) <1 0 0> <0 0 1> 0.020 151.8
Ga2O3 (mp-886) <1 0 0> <0 0 1> 0.020 341.7
Ni (mp-23) <1 1 0> <0 1 0> 0.024 332.1
Te2Mo (mp-602) <1 1 0> <0 0 1> 0.028 189.8
MoSe2 (mp-1634) <0 0 1> <0 1 0> 0.030 332.1
WSe2 (mp-1821) <0 0 1> <0 1 0> 0.030 332.1
SiC (mp-7631) <1 0 0> <0 0 1> 0.032 189.8
CdWO4 (mp-19387) <1 0 1> <0 1 0> 0.032 221.4
Mg (mp-153) <0 0 1> <0 0 1> 0.033 303.7
DyScO3 (mp-31120) <1 0 0> <1 0 0> 0.036 91.1
TiO2 (mp-390) <1 0 0> <0 1 0> 0.038 110.7
NdGaO3 (mp-3196) <1 1 1> <1 0 0> 0.038 273.4
LaAlO3 (mp-2920) <0 0 1> <0 1 0> 0.041 332.1
CsI (mp-614603) <1 1 0> <0 0 1> 0.043 265.7
SiC (mp-11714) <1 0 0> <0 0 1> 0.046 189.8
WS2 (mp-224) <1 0 1> <0 0 1> 0.047 227.8
TbScO3 (mp-31119) <1 0 0> <1 0 0> 0.055 91.1
AlN (mp-661) <1 0 1> <1 1 0> 0.058 106.6
NdGaO3 (mp-3196) <0 0 1> <0 0 1> 0.059 341.7
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.061 303.7
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.061 189.8
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.061 189.8
WS2 (mp-224) <0 0 1> <0 0 1> 0.061 303.7
C (mp-48) <1 0 1> <0 0 1> 0.063 303.7
WS2 (mp-224) <1 0 0> <0 1 1> 0.067 134.2
InP (mp-20351) <1 1 0> <0 1 1> 0.069 201.3
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.071 273.4
TiO2 (mp-390) <0 0 1> <0 1 0> 0.073 221.4
BaTiO3 (mp-5986) <1 0 0> <0 0 1> 0.074 265.7
MgF2 (mp-1249) <1 1 1> <0 1 1> 0.076 268.5
Ni (mp-23) <1 0 0> <0 0 1> 0.077 303.7
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.091 341.7
TePb (mp-19717) <1 1 0> <1 0 0> 0.094 182.3
TeO2 (mp-2125) <1 1 0> <1 0 1> 0.096 98.7
Ag (mp-124) <1 0 0> <1 0 0> 0.097 273.4
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.097 189.8
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.100 182.3
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.101 273.4
Ge (mp-32) <1 1 0> <0 1 0> 0.102 276.7
CdS (mp-672) <1 1 0> <0 1 1> 0.102 201.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
34 14 10 0 0 0
14 24 12 0 0 0
10 12 26 0 0 0
0 0 0 11 0 0
0 0 0 0 8 0
0 0 0 0 0 6
Compliance Tensor Sij (10-12Pa-1)
38.3 -18.5 -6 0 0 0
-18.5 63.2 -23.1 0 0 0
-6 -23.1 51.6 0 0 0
0 0 0 88.3 0 0
0 0 0 0 128 0
0 0 0 0 0 165.5
Shear Modulus GV
8 GPa
Bulk Modulus KV
17 GPa
Shear Modulus GR
8 GPa
Bulk Modulus KR
17 GPa
Shear Modulus GVRH
8 GPa
Bulk Modulus KVRH
17 GPa
Elastic Anisotropy
0.39
Poisson's Ratio
0.30

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
3.09 0.00 0.00
0.00 3.06 0.00
0.00 0.00 3.09
Dielectric Tensor εij (total)
6.70 0.00 0.00
0.00 7.03 0.00
0.00 0.00 6.89
Polycrystalline dielectric constant εpoly
(electronic contribution)
3.08
Polycrystalline dielectric constant εpoly
(total)
6.87
Refractive Index n
1.76
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TiOF (mp-752496) 0.4984 0.072 3
TaNO (mp-4165) 0.5268 0.000 3
CeZr11O24 (mp-752706) 0.5343 0.016 3
VOF (mp-764286) 0.5198 0.030 3
DySCl (mp-561307) 0.5131 0.000 3
ZrO2 (mp-755089) 0.2744 0.022 2
NbO2 (mp-776975) 0.4327 0.072 2
SrI2 (mp-568284) 0.3399 0.000 2
CeSe2 (mp-1080303) 0.5232 0.024 2
CeSe2 (mp-1080853) 0.4863 0.026 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
700 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Sr_sv Br
Final Energy/Atom
-3.8036 eV
Corrected Energy
-49.9150 eV
Uncorrected energy = -45.6430 eV Composition-based energy adjustment (-0.534 eV/atom x 8.0 atoms) = -4.2720 eV Corrected energy = -49.9150 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 15972
Submitted by
User remarks:
  • Strontium bromide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)