Final Magnetic Moment0.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.065 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.390 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.23 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToZr2Al3C4 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63mc [186] |
HallP 6c 2c |
Point Group6mm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 172.8 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 227.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 291.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 109.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 272.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 254.6 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 127.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 90.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 163.7 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 327.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 172.8 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 9.1 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 181.8 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 136.4 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 90.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 318.2 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 281.9 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 151.3 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 318.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 63.6 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 200.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 318.2 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 145.5 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 174.3 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 291.0 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 281.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 90.9 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 218.2 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 54.6 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 54.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 218.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 190.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 63.6 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 163.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 327.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 172.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 81.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 27.3 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 200.0 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 163.7 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 63.6 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 318.2 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 318.2 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 81.8 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 163.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 27.3 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 254.6 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 227.3 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 327.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 318.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zr_sv Al C |
Final Energy/Atom-7.3138 eV |
Corrected Energy-131.6485 eV
-131.6485 eV = -131.6485 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)