Final Magnetic Moment5.483 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-0.168 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.65 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI41/amd [141] |
HallI 4bw 2bw 1bw |
Point Group4/mmm |
Crystal Systemtetragonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 78.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 314.6 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 78.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 78.6 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 157.3 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 0> | 188.1 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 188.1 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 314.6 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 235.9 |
GdScO3 (mp-5690) | <1 1 0> | <0 0 1> | 314.6 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 314.6 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 314.6 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 78.6 |
BaTiO3 (mp-5986) | <0 0 1> | <0 0 1> | 78.6 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 314.6 |
Au (mp-81) | <1 0 0> | <0 0 1> | 157.3 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 157.3 |
CaCO3 (mp-3953) | <1 1 0> | <0 0 1> | 157.3 |
YAlO3 (mp-3792) | <1 0 1> | <0 0 1> | 235.9 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <0 0 1> | 157.3 |
TbScO3 (mp-31119) | <1 1 0> | <0 0 1> | 314.6 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 78.6 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 314.6 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 235.9 |
MgF2 (mp-1249) | <1 1 1> | <0 0 1> | 235.9 |
SrTiO3 (mp-4651) | <0 0 1> | <0 0 1> | 157.3 |
YAlO3 (mp-3792) | <1 1 1> | <1 0 0> | 188.1 |
CaF2 (mp-2741) | <1 0 0> | <0 0 1> | 157.3 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 78.6 |
SrTiO3 (mp-4651) | <1 1 0> | <0 0 1> | 314.6 |
ZnTe (mp-2176) | <1 0 0> | <0 0 1> | 78.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pu Zn |
Final Energy/Atom-2.9885 eV |
Corrected Energy-149.4254 eV
-149.4254 eV = -149.4254 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)