Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.044 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.63 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP62c [190] |
HallP 6c 2c |
Point Group6m2 |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 209.0 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 156.8 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 261.3 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 209.0 |
LiF (mp-1138) | <1 1 1> | <1 1 1> | 201.7 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 222.3 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 222.3 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 52.3 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 90.5 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 209.0 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 209.0 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 311.2 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 44.5 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 222.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 222.3 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 261.3 |
BN (mp-984) | <0 0 1> | <1 0 0> | 261.3 |
BN (mp-984) | <1 0 0> | <1 0 0> | 156.8 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 311.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 44.5 |
MoS2 (mp-1434) | <1 0 0> | <1 1 0> | 271.5 |
Al (mp-134) | <1 0 0> | <1 0 0> | 209.0 |
Al (mp-134) | <1 1 0> | <1 0 0> | 209.0 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 261.3 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 311.2 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 261.3 |
TeO2 (mp-2125) | <0 1 0> | <1 1 0> | 271.5 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 133.4 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 311.2 |
Fe3O4 (mp-19306) | <1 0 0> | <0 0 1> | 222.3 |
Fe3O4 (mp-19306) | <1 1 1> | <0 0 1> | 133.4 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 222.3 |
MgO (mp-1265) | <1 1 0> | <0 0 1> | 311.2 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 133.4 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 177.8 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 209.0 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 133.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 156.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 261.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 261.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 177.8 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 311.2 |
C (mp-66) | <1 0 0> | <1 0 0> | 52.3 |
C (mp-66) | <1 1 0> | <0 0 1> | 222.3 |
C (mp-66) | <1 1 1> | <1 0 0> | 261.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 222.3 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 313.5 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 271.5 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 271.5 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 261.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HfCoSn (mp-22315) | 0.2703 | 0.000 | 3 |
ZrGaPt (mp-601253) | 0.3284 | 0.000 | 3 |
HfAlPt (mp-571619) | 0.1909 | 0.000 | 3 |
ScGeOs (mp-1078635) | 0.3817 | 0.000 | 3 |
HfGaNi (mp-1079860) | 0.3800 | 0.000 | 3 |
TaNi2TeSe (mp-622009) | 0.7270 | 0.000 | 4 |
Mg3Al8FeSi6 (mp-571315) | 0.6636 | 0.141 | 4 |
USe2 (mp-8591) | 0.5206 | 0.032 | 2 |
US2 (mp-669500) | 0.5432 | 0.000 | 2 |
GePd2 (mp-423) | 0.5096 | 0.000 | 2 |
K2Re (mp-1080778) | 0.5180 | 1.993 | 2 |
K2Tc (mp-1084834) | 0.4882 | 1.575 | 2 |
Rb (mp-640416) | 0.7382 | 0.057 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Zr_sv Al Pt |
Final Energy/Atom-7.1649 eV |
Corrected Energy-128.9687 eV
-128.9687 eV = -128.9687 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)