Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNon-magnetic |
Formation Energy / Atom-0.441 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.009 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.06 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToICl |
Band Gap1.469 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 0> | 229.5 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 248.9 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 229.5 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 226.7 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 224.5 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 151.1 |
SiO2 (mp-6930) | <1 1 1> | <1 0 -1> | 105.4 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 226.7 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 317.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 226.7 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 210.7 |
CdS (mp-672) | <1 0 0> | <1 0 1> | 113.5 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 302.3 |
LiF (mp-1138) | <1 1 0> | <1 0 -1> | 210.7 |
Te2W (mp-22693) | <0 1 1> | <0 0 1> | 302.3 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 317.2 |
Ag (mp-124) | <1 0 0> | <1 0 -1> | 105.4 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 317.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 302.3 |
LiNbO3 (mp-3731) | <1 0 0> | <0 1 1> | 224.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 302.3 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 0 0> | 317.2 |
Al (mp-134) | <1 1 0> | <1 0 -1> | 210.7 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 248.9 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 -1> | 210.7 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 317.2 |
TeO2 (mp-2125) | <0 1 0> | <1 0 -1> | 210.7 |
TeO2 (mp-2125) | <1 0 0> | <1 0 -1> | 210.7 |
TeO2 (mp-2125) | <0 1 1> | <1 0 1> | 227.1 |
TeO2 (mp-2125) | <1 0 1> | <1 0 1> | 227.1 |
Fe3O4 (mp-19306) | <1 1 0> | <1 0 -1> | 105.4 |
C (mp-66) | <1 1 1> | <0 0 1> | 226.7 |
Mg (mp-153) | <1 0 1> | <1 0 0> | 317.2 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 1 1> | 224.5 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 151.1 |
KP(HO2)2 (mp-23959) | <0 0 1> | <0 1 1> | 224.5 |
InP (mp-20351) | <1 1 0> | <0 0 1> | 151.1 |
Ni (mp-23) | <1 1 0> | <1 0 -1> | 105.4 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 317.2 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 226.7 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 237.9 |
BaTiO3 (mp-5986) | <1 1 0> | <1 0 -1> | 210.7 |
NdGaO3 (mp-3196) | <1 0 1> | <1 0 0> | 158.6 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 302.3 |
SiC (mp-11714) | <1 0 1> | <1 0 1> | 227.1 |
MoSe2 (mp-1634) | <0 0 1> | <0 1 0> | 248.9 |
Ga2O3 (mp-886) | <1 0 0> | <0 0 1> | 302.3 |
Au (mp-81) | <1 0 0> | <1 0 -1> | 105.4 |
Au (mp-81) | <1 1 0> | <1 0 0> | 317.2 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 226.7 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Br2O (mp-28460) | 0.3961 | 0.047 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points16 |
U Values-- |
PseudopotentialsVASP PAW: I Cl |
Final Energy/Atom-1.8279 eV |
Corrected Energy-29.2464 eV
-29.2464 eV = -29.2464 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)