Final Magnetic Moment0.007 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.588 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.050 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.23 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNd(NiSb)2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationTI*
|
SubclassificationSEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 0> | 198.3 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 133.1 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 95.1 |
AlN (mp-661) | <1 0 1> | <1 0 1> | 201.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 323.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 285.2 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 171.1 |
BaF2 (mp-1029) | <1 1 1> | <1 0 1> | 201.8 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 140.2 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 132.2 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 152.1 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 233.7 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 152.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 152.1 |
SiO2 (mp-6930) | <1 1 0> | <0 0 1> | 342.2 |
SiO2 (mp-6930) | <1 1 1> | <1 1 1> | 206.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 252.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 280.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 327.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 38.0 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 266.2 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 187.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 190.1 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 233.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 247.2 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 264.4 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 323.2 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 171.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 361.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 38.0 |
InAs (mp-20305) | <1 1 1> | <1 0 1> | 201.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 171.1 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 302.7 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 327.2 |
Te2W (mp-22693) | <1 0 1> | <1 1 0> | 198.3 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 228.1 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 285.2 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 152.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 302.7 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 206.3 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 171.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 152.1 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 66.1 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 233.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 247.2 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 247.2 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 66.1 |
Te2Mo (mp-602) | <1 0 0> | <1 0 0> | 327.2 |
BN (mp-984) | <1 0 1> | <0 0 1> | 304.2 |
BN (mp-984) | <1 1 1> | <0 0 1> | 133.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
La(NiAs)2 (mp-5982) | 0.0638 | 0.034 | 3 |
Gd(NiSb)2 (mp-569296) | 0.0577 | 0.097 | 3 |
Sm(NiSb)2 (mp-568599) | 0.0214 | 0.054 | 3 |
Pr(NiSb)2 (mp-568703) | 0.0727 | 0.048 | 3 |
Eu(NiSb)2 (mp-570308) | 0.0397 | 0.000 | 3 |
La3Cu4(P2O)2 (mp-6309) | 0.5327 | 0.000 | 4 |
EuGa4 (mp-21884) | 0.3303 | 0.000 | 2 |
ThZn4 (mp-536) | 0.3180 | 0.000 | 2 |
SrGa4 (mp-1827) | 0.3283 | 0.000 | 2 |
BaIn4 (mp-22687) | 0.3402 | 0.000 | 2 |
BaGa4 (mp-335) | 0.2951 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nd_3 Ni_pv Sb |
Final Energy/Atom-5.5051 eV |
Corrected Energy-27.9095 eV
Uncorrected energy = -27.5255 eV
Composition-based energy adjustment (-0.192 eV/atom x 2.0 atoms) = -0.3840 eV
Corrected energy = -27.9095 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)