@article{Kuhn1975, author = "Kuhn, A. and Chevalier, R. and Rimsky, A.", title = "Atomic structure of a 4H GaSe polytype named delta-type", journal = "Acta Crystallographica B (24,1968-38,1982)", year = "1975", volume = "31", pages = "2841-2842", ASTM_id = "ACBCAR" }