Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.254 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.006 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density13.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTa3Ga2 + Ta |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mcm [140] |
Hall-I 4 2c |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 263.9 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 223.9 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 316.7 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 158.3 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 223.9 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 223.9 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 223.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 263.9 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 211.1 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 149.3 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 263.9 |
SiO2 (mp-6930) | <0 0 1> | <1 1 0> | 223.9 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 211.1 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 223.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 263.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 263.9 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 263.9 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 211.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 211.1 |
LiF (mp-1138) | <1 1 1> | <1 0 1> | 118.0 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 223.9 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 263.9 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 223.9 |
Ag (mp-124) | <1 1 1> | <1 0 1> | 118.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 316.7 |
BN (mp-984) | <1 0 1> | <1 0 0> | 263.9 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 105.6 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 298.5 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 223.9 |
BN (mp-984) | <0 0 1> | <1 0 0> | 263.9 |
BN (mp-984) | <1 0 0> | <1 0 0> | 158.3 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 0> | 74.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 211.1 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 211.1 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 263.9 |
Al (mp-134) | <1 0 0> | <1 0 0> | 211.1 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 263.9 |
LiTaO3 (mp-3666) | <1 0 0> | <1 0 0> | 211.1 |
MgO (mp-1265) | <1 1 1> | <1 0 0> | 211.1 |
SiC (mp-7631) | <1 0 1> | <1 0 1> | 236.0 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 105.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 1> | 236.0 |
C (mp-66) | <1 1 0> | <1 0 1> | 236.0 |
C (mp-66) | <1 1 1> | <1 1 0> | 223.9 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 298.5 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 263.9 |
Mg (mp-153) | <1 0 0> | <1 1 0> | 149.3 |
Mg (mp-153) | <1 1 0> | <1 1 0> | 223.9 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 1 0> | 223.9 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 149.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Nb5SiSn2 (mp-7557) | 0.4843 | 0.001 | 3 |
Ti5FeSb2 (mp-30326) | 0.6069 | 0.022 | 3 |
Ti5Sb2Rh (mp-16687) | 0.3384 | 0.030 | 3 |
Ti5CuSb2 (mp-13020) | 0.2711 | 0.001 | 3 |
Nb5GaSn2 (mp-17230) | 0.3156 | 0.000 | 3 |
Ta5Ge3 (mp-17615) | 0.1458 | 0.016 | 2 |
Nb5Ga3 (mp-570293) | 0.1165 | 0.008 | 2 |
Nb5Ge3 (mp-16842) | 0.0981 | 0.000 | 2 |
Nb5Si3 (mp-567996) | 0.1403 | 0.045 | 2 |
V5Si3 (mp-568671) | 0.1201 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ta_pv Ga_d |
Final Energy/Atom-8.8011 eV |
Corrected Energy-140.8182 eV
-140.8182 eV = -140.8182 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)