Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.343 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.022 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.26 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToK3Bi |
Band Gap0.129 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 152.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 304.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 76.1 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 107.7 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 107.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 304.5 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 76.1 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 107.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 304.5 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 152.3 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 215.3 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 131.9 |
TeO2 (mp-2125) | <1 0 0> | <1 1 0> | 215.3 |
TeO2 (mp-2125) | <1 1 0> | <1 0 0> | 304.5 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 76.1 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 107.7 |
Fe3O4 (mp-19306) | <1 1 1> | <1 1 1> | 131.9 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 304.5 |
TiO2 (mp-2657) | <1 1 1> | <1 0 0> | 228.4 |
C (mp-66) | <1 1 0> | <1 1 0> | 107.7 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 304.5 |
LaF3 (mp-905) | <0 0 1> | <1 0 0> | 228.4 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 152.3 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 304.5 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 304.5 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 76.1 |
PbSe (mp-2201) | <1 1 0> | <1 1 0> | 107.7 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 152.3 |
BaTiO3 (mp-5986) | <1 1 0> | <1 1 0> | 215.3 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 304.5 |
Ga2O3 (mp-886) | <1 0 -1> | <1 1 1> | 263.7 |
Ga2O3 (mp-886) | <1 1 0> | <1 1 0> | 215.3 |
Si (mp-149) | <1 0 0> | <1 0 0> | 152.3 |
Au (mp-81) | <1 0 0> | <1 1 1> | 263.7 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 76.1 |
CdSe (mp-2691) | <1 1 0> | <1 1 0> | 107.7 |
C (mp-48) | <0 0 1> | <1 1 1> | 131.9 |
CaCO3 (mp-3953) | <1 1 0> | <1 0 0> | 152.3 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 152.3 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 76.1 |
SiC (mp-8062) | <1 1 0> | <1 1 0> | 107.7 |
SiC (mp-8062) | <1 1 1> | <1 1 1> | 131.9 |
CsI (mp-614603) | <1 0 0> | <1 0 0> | 304.5 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 76.1 |
GaSb (mp-1156) | <1 1 0> | <1 1 0> | 107.7 |
SrTiO3 (mp-4651) | <0 0 1> | <1 0 0> | 152.3 |
SrTiO3 (mp-4651) | <1 1 0> | <1 0 0> | 304.5 |
Cu (mp-30) | <1 1 1> | <1 0 0> | 228.4 |
Ge (mp-32) | <1 0 0> | <1 0 0> | 304.5 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 152.3 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
44 | 26 | 26 | 0 | 0 | 0 |
26 | 44 | 26 | 0 | 0 | 0 |
26 | 26 | 44 | 0 | 0 | 0 |
0 | 0 | 0 | 34 | 0 | 0 |
0 | 0 | 0 | 0 | 34 | 0 |
0 | 0 | 0 | 0 | 0 | 34 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
39.7 | -14.6 | -14.6 | 0 | 0 | 0 |
-14.6 | 39.7 | -14.6 | 0 | 0 | 0 |
-14.6 | -14.6 | 39.7 | 0 | 0 | 0 |
0 | 0 | 0 | 29.7 | 0 | 0 |
0 | 0 | 0 | 0 | 29.7 | 0 |
0 | 0 | 0 | 0 | 0 | 29.7 |
Shear Modulus GV24 GPa |
Bulk Modulus KV32 GPa |
Shear Modulus GR16 GPa |
Bulk Modulus KR32 GPa |
Shear Modulus GVRH20 GPa |
Bulk Modulus KVRH32 GPa |
Elastic Anisotropy2.32 |
Poisson's Ratio0.24 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YInAg2 (mp-569823) | 0.0000 | 0.000 | 3 |
ZrInAu2 (mp-581707) | 0.0000 | 0.012 | 3 |
Ba2NbO (mp-34023) | 0.0000 | 1.725 | 3 |
LaInAg2 (mp-568917) | 0.0000 | 0.000 | 3 |
Li2GaIr (mp-570528) | 0.0000 | 0.217 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.058 | 4 |
LiMgSbPt (mp-571584) | 0.0000 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
Cs3Bi (mp-635413) | 0.0000 | 0.000 | 2 |
MnS (mp-556853) | 0.0000 | 0.501 | 2 |
YCd3 (mp-571059) | 0.0000 | 0.020 | 2 |
Rb3Sb (mp-33018) | 0.0000 | 0.032 | 2 |
Br3N (mp-36891) | 0.0000 | 1.872 | 2 |
Br (mp-673171) | 0.0000 | 0.630 | 1 |
Ti (mp-73) | 0.0000 | 0.112 | 1 |
I (mp-684663) | 0.0000 | 0.446 | 1 |
Zr (mp-41) | 0.0000 | 0.075 | 1 |
Cr (mp-90) | 0.0000 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: K_sv Bi |
Final Energy/Atom-2.1482 eV |
Corrected Energy-8.5927 eV
-8.5927 eV = -8.5927 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)