material

Cd(InSe2)2

ID:

mp-568661

DOI:

10.17188/1272600


Tags: Cadmium indium selenide (1/2/4) Cadmium diindium selenide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.571 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.003 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.18 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Cd(InSe2)2
Band Gap
1.226 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I42m [121]
Hall
I 4 2
Point Group
42m
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 151955 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Al (mp-134) <1 0 0> <0 0 1> 0.000 277.4
TiO2 (mp-2657) <0 0 1> <0 0 1> 0.001 173.4
Ag (mp-124) <1 0 0> <0 0 1> 0.001 34.7
Au (mp-81) <1 0 0> <0 0 1> 0.004 34.7
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.005 312.1
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.005 277.4
SiC (mp-8062) <1 0 0> <0 0 1> 0.006 173.4
TePb (mp-19717) <1 0 0> <0 0 1> 0.008 173.4
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.010 277.4
Ag (mp-124) <1 1 1> <1 0 1> 0.010 238.7
PbSe (mp-2201) <1 0 0> <0 0 1> 0.011 312.1
Mg (mp-153) <1 0 1> <0 0 1> 0.016 208.0
ZrO2 (mp-2858) <0 0 1> <0 0 1> 0.019 138.7
GaSb (mp-1156) <1 0 0> <0 0 1> 0.022 312.1
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.026 173.4
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.028 277.4
GaN (mp-804) <1 0 1> <0 0 1> 0.028 208.0
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.029 242.7
Au (mp-81) <1 1 1> <1 0 1> 0.031 238.7
CsI (mp-614603) <1 0 0> <0 0 1> 0.032 312.1
CdSe (mp-2691) <1 0 0> <0 0 1> 0.033 312.1
SiC (mp-11714) <1 0 0> <0 0 1> 0.039 346.7
BaF2 (mp-1029) <1 0 0> <0 0 1> 0.044 312.1
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.049 277.4
Ga2O3 (mp-886) <1 0 0> <1 0 0> 0.057 71.6
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.058 138.7
CdTe (mp-406) <1 0 0> <0 0 1> 0.059 173.4
CdS (mp-672) <0 0 1> <0 0 1> 0.059 242.7
Ni (mp-23) <1 0 0> <0 0 1> 0.060 312.1
InSb (mp-20012) <1 0 0> <0 0 1> 0.070 173.4
ZnO (mp-2133) <0 0 1> <0 0 1> 0.073 346.7
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.073 312.1
InAs (mp-20305) <1 1 0> <1 0 0> 0.075 214.9
ZnTe (mp-2176) <1 1 0> <1 0 0> 0.079 214.9
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.079 69.3
GaP (mp-2490) <1 0 0> <0 0 1> 0.080 277.4
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.085 173.4
GaN (mp-804) <1 1 1> <0 0 1> 0.090 277.4
SiC (mp-8062) <1 1 0> <1 0 0> 0.091 214.9
BaTiO3 (mp-5986) <1 0 0> <1 1 0> 0.091 101.3
LiF (mp-1138) <1 1 1> <0 0 1> 0.091 173.4
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.095 173.4
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.095 173.4
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.100 312.1
TbScO3 (mp-31119) <1 0 0> <0 0 1> 0.100 138.7
BN (mp-984) <0 0 1> <0 0 1> 0.101 346.7
MgAl2O4 (mp-3536) <1 1 0> <1 0 0> 0.101 286.5
TeO2 (mp-2125) <0 1 0> <1 1 0> 0.101 202.6
BN (mp-984) <1 0 0> <1 0 0> 0.103 286.5
GdScO3 (mp-5690) <1 0 0> <0 0 1> 0.106 138.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
39 26 17 0 0 0
26 39 17 0 0 0
17 17 35 0 0 0
0 0 0 17 0 0
0 0 0 0 17 0
0 0 0 0 0 27
Compliance Tensor Sij (10-12Pa-1)
48.5 -27.8 -9.8 0 0 0
-27.8 48.5 -9.8 0 0 0
-9.8 -9.8 37.8 0 0 0
0 0 0 58.2 0 0
0 0 0 0 58.2 0
0 0 0 0 0 37.5
Shear Modulus GV
16 GPa
Bulk Modulus KV
26 GPa
Shear Modulus GR
13 GPa
Bulk Modulus KR
25 GPa
Shear Modulus GVRH
14 GPa
Bulk Modulus KVRH
25 GPa
Elastic Anisotropy
1.28
Poisson's Ratio
0.27

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.15826 0.00000 0.00000
0.00000 0.00000 0.00000 0.00000 0.15826 0.00000
0.00000 0.00000 0.00000 0.00000 0.00000 0.15926
Piezoelectric Modulus ‖eijmax
0.15926 C/m2
Crystallographic Direction vmax
0.00000
0.00000
1.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
7.70 0.00 0.00
0.00 7.70 0.00
0.00 0.00 7.38
Dielectric Tensor εij (total)
11.53 0.00 0.00
0.00 11.53 0.00
0.00 0.00 11.35
Polycrystalline dielectric constant εpoly
(electronic contribution)
7.59
Polycrystalline dielectric constant εpoly
(total)
11.47
Refractive Index n
2.76
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sn(HgSe2)2 (mp-10955) 0.1393 0.000 3
Cd(InSe2)2 (mp-568032) 0.1210 0.004 3
In5AgSe8 (mp-571103) 0.1631 0.000 3
Zn(InSe2)2 (mp-22607) 0.1895 0.000 3
Zn(InTe2)2 (mp-20832) 0.1379 0.000 3
CaZnSO (mp-7204) 0.4258 0.010 4
Li2Ga2GeS6 (mp-554782) 0.7186 0.035 4
ZnAgPS4 (mp-558807) 0.6188 0.000 4
CaFeSO (mp-1078415) 0.4523 0.224 4
ZnCu4(SnSe4)2 (mvc-14983) 0.5438 0.035 4
Ge3As4 (mp-569600) 0.4478 0.041 2
GeAs (mp-9548) 0.4814 0.002 2
As4C3 (mp-568505) 0.2672 0.874 2
Si3As4 (mp-570744) 0.3676 0.059 2
GeP (mp-1095275) 0.4548 0.015 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Cd In_d Se
Final Energy/Atom
-3.4846 eV
Corrected Energy
-26.2803 eV
Uncorrected energy = -24.3923 eV Composition-based energy adjustment (-0.472 eV/atom x 4.0 atoms) = -1.8880 eV Corrected energy = -26.2803 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 151955
  • 620044
Submitted by
User remarks:
  • Cadmium diindium selenide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)