material

V5Si3

ID:

mp-568671

DOI:

10.17188/1274636


Tags: Vanadium silicide (5/3)

Material Details

Final Magnetic Moment
0.004 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.585 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
5.38 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mcm [140]
Hall
-I 4 2c
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 652495 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
InP (mp-20351) <1 0 0> <0 0 1> 0.008 176.9
InSb (mp-20012) <1 1 0> <1 0 0> 0.012 311.4
CdTe (mp-406) <1 1 0> <1 0 0> 0.016 311.4
LiF (mp-1138) <1 1 0> <1 1 0> 0.018 188.7
MgAl2O4 (mp-3536) <1 1 0> <1 1 0> 0.019 188.7
InSb (mp-20012) <1 0 0> <0 0 1> 0.028 88.5
Ni (mp-23) <1 0 0> <1 0 0> 0.033 222.4
Ge (mp-32) <1 1 0> <1 1 0> 0.036 188.7
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.043 222.4
CdTe (mp-406) <1 0 0> <0 0 1> 0.043 88.5
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.077 222.4
CeO2 (mp-20194) <1 1 0> <1 1 0> 0.081 125.8
LiNbO3 (mp-3731) <1 0 0> <1 0 1> 0.083 297.0
Si (mp-149) <1 1 0> <1 1 0> 0.088 125.8
GaAs (mp-2534) <1 1 0> <1 1 0> 0.091 188.7
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.098 44.5
ZnO (mp-2133) <1 0 0> <1 0 1> 0.102 297.0
SiC (mp-11714) <1 0 0> <1 1 1> 0.105 217.1
LiGaO2 (mp-5854) <0 0 1> <1 1 0> 0.111 251.6
MgF2 (mp-1249) <1 0 1> <1 0 0> 0.126 133.5
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.142 188.7
Te2W (mp-22693) <0 0 1> <1 0 1> 0.182 198.0
LaAlO3 (mp-2920) <1 0 0> <1 1 1> 0.193 217.1
TiO2 (mp-390) <1 0 1> <1 0 1> 0.245 198.0
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.254 311.4
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.261 222.4
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.263 311.4
LaAlO3 (mp-2920) <1 1 1> <1 1 0> 0.264 125.8
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.265 311.4
CdS (mp-672) <0 0 1> <1 0 0> 0.266 311.4
NdGaO3 (mp-3196) <1 0 1> <0 0 1> 0.272 265.4
Au (mp-81) <1 0 0> <0 0 1> 0.281 88.5
LaAlO3 (mp-2920) <1 1 0> <1 1 0> 0.291 125.8
ZnO (mp-2133) <1 1 0> <1 0 1> 0.314 297.0
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.331 125.8
GaN (mp-804) <1 1 0> <1 0 1> 0.345 297.0
MgO (mp-1265) <1 0 0> <1 0 0> 0.351 89.0
PbS (mp-21276) <1 0 0> <0 0 1> 0.352 176.9
TiO2 (mp-2657) <1 0 0> <1 1 0> 0.361 125.8
Mg (mp-153) <1 0 0> <1 0 1> 0.377 99.0
Mg (mp-153) <0 0 1> <1 0 0> 0.394 311.4
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.428 44.5
TePb (mp-19717) <1 1 0> <1 0 0> 0.443 311.4
Mg (mp-153) <1 0 1> <1 0 0> 0.450 222.4
LaAlO3 (mp-2920) <0 0 1> <1 1 0> 0.456 125.8
Bi2Te3 (mp-34202) <0 0 1> <1 1 0> 0.458 314.6
Cu (mp-30) <1 1 1> <1 1 0> 0.464 314.6
Al (mp-134) <1 1 0> <1 1 0> 0.472 188.7
YAlO3 (mp-3792) <0 0 1> <1 0 0> 0.480 222.4
Al2O3 (mp-1143) <1 0 0> <1 1 0> 0.494 62.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
355 96 96 0 0 0
96 402 102 0 0 0
96 102 402 0 0 0
0 0 0 127 0 0
0 0 0 0 97 0
0 0 0 0 0 97
Compliance Tensor Sij (10-12Pa-1)
3.1 -0.6 -0.6 0 0 0
-0.6 2.8 -0.6 0 0 0
-0.6 -0.6 2.8 0 0 0
0 0 0 7.9 0 0
0 0 0 0 10.3 0
0 0 0 0 0 10.3
Shear Modulus GV
122 GPa
Bulk Modulus KV
194 GPa
Shear Modulus GR
118 GPa
Bulk Modulus KR
193 GPa
Shear Modulus GVRH
120 GPa
Bulk Modulus KVRH
194 GPa
Elastic Anisotropy
0.17
Poisson's Ratio
0.24

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Nb5SiSn2 (mp-7557) 0.5208 0.001 3
Ti2InNi2 (mp-20339) 0.6339 0.000 3
Ti5Sb2Rh (mp-16687) 0.4111 0.030 3
Ti5CuSb2 (mp-13020) 0.3458 0.001 3
Nb5GaSn2 (mp-17230) 0.3540 0.000 3
Si3W5 (mp-31219) 0.1453 0.020 2
Ta5Ge3 (mp-17615) 0.0959 0.016 2
Ta5Ga3 (mp-568376) 0.1201 0.006 2
Si3Mo5 (mp-1332) 0.1029 0.000 2
Nb5Ge3 (mp-16842) 0.0898 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: V_pv Si
Final Energy/Atom
-8.2950 eV
Corrected Energy
-132.7207 eV
-132.7207 eV = -132.7207 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 652495
  • 652485
  • 652527
  • 652506
Submitted by
User remarks:
  • Vanadium silicide (5/3)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)