material

VPd3

ID:

mp-568711

DOI:

10.17188/1274655


Tags: Palladium vanadium (3/1) - LT

Material Details

Final Magnetic Moment
1.234 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
FM
Formation Energy / Atom
-0.237 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.011 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
10.32 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
VPd3
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
MoS2 (mp-1434) <0 0 1> <1 1 1> 0.002 26.4
WS2 (mp-224) <0 0 1> <1 1 1> 0.002 26.4
InAs (mp-20305) <1 0 0> <1 0 0> 0.004 76.3
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.006 30.5
CaF2 (mp-2741) <1 1 0> <1 1 0> 0.006 43.1
InP (mp-20351) <1 1 1> <1 1 1> 0.009 184.9
Mg (mp-153) <0 0 1> <1 1 1> 0.009 26.4
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.010 76.3
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.012 137.3
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.013 61.0
Mg (mp-153) <1 0 0> <1 1 0> 0.014 151.0
WS2 (mp-224) <1 1 1> <1 1 1> 0.020 79.2
MoS2 (mp-1434) <1 1 1> <1 1 0> 0.023 237.3
KCl (mp-23193) <1 1 0> <1 1 0> 0.031 172.5
C (mp-48) <1 0 0> <1 1 0> 0.032 172.5
GaP (mp-2490) <1 0 0> <1 0 0> 0.033 30.5
SiC (mp-8062) <1 0 0> <1 0 0> 0.034 76.3
GaP (mp-2490) <1 1 0> <1 1 0> 0.035 43.1
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.036 137.3
Ge(Bi3O5)4 (mp-23352) <1 1 1> <1 1 1> 0.044 184.9
MoS2 (mp-1434) <1 1 0> <1 1 0> 0.059 237.3
Bi2Se3 (mp-541837) <0 0 1> <1 1 1> 0.062 105.7
Mg (mp-153) <1 1 0> <1 1 0> 0.065 86.3
Ni (mp-23) <1 0 0> <1 0 0> 0.068 61.0
TiO2 (mp-2657) <1 0 1> <1 1 0> 0.071 129.4
WS2 (mp-224) <1 1 0> <1 1 0> 0.071 237.3
Ag (mp-124) <1 0 0> <1 0 0> 0.073 137.3
Ag (mp-124) <1 1 0> <1 1 0> 0.077 194.1
Al2O3 (mp-1143) <0 0 1> <1 1 1> 0.085 79.2
GaN (mp-804) <1 0 0> <1 1 0> 0.096 151.0
MoSe2 (mp-1634) <1 0 0> <1 1 0> 0.102 258.8
NdGaO3 (mp-3196) <0 1 1> <1 1 1> 0.104 52.8
Mg (mp-153) <1 1 1> <1 1 1> 0.106 211.3
TbScO3 (mp-31119) <0 1 1> <1 1 0> 0.111 107.8
Te2W (mp-22693) <0 0 1> <1 0 0> 0.125 335.5
YVO4 (mp-19133) <1 0 0> <1 1 1> 0.138 184.9
NdGaO3 (mp-3196) <0 1 0> <1 1 0> 0.139 43.1
CdSe (mp-2691) <1 0 0> <1 0 0> 0.140 76.3
CsI (mp-614603) <1 0 0> <1 0 0> 0.143 61.0
Bi2Te3 (mp-34202) <0 0 1> <1 1 0> 0.151 86.3
Fe2O3 (mp-24972) <0 0 1> <1 1 0> 0.152 345.1
CsI (mp-614603) <1 1 0> <1 1 0> 0.152 86.3
CsI (mp-614603) <1 1 1> <1 1 1> 0.156 105.7
PbS (mp-21276) <1 1 1> <1 1 1> 0.162 184.9
YAlO3 (mp-3792) <0 1 1> <1 0 0> 0.162 289.8
CaCO3 (mp-3953) <1 1 0> <1 0 0> 0.167 152.5
SiO2 (mp-6930) <1 1 0> <1 1 0> 0.173 194.1
ZnO (mp-2133) <0 0 1> <1 0 0> 0.182 167.8
ZrO2 (mp-2858) <1 1 -1> <1 1 0> 0.182 323.5
Au (mp-81) <1 0 0> <1 0 0> 0.183 137.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
254 143 143 0 0 0
143 254 143 0 0 0
143 143 255 0 0 0
0 0 0 107 0 0
0 0 0 0 107 0
0 0 0 0 0 107
Compliance Tensor Sij (10-12Pa-1)
6.6 -2.4 -2.4 0 0 0
-2.4 6.6 -2.4 0 0 0
-2.4 -2.4 6.6 0 0 0
0 0 0 9.4 0 0
0 0 0 0 9.4 0
0 0 0 0 0 9.4
Shear Modulus GV
86 GPa
Bulk Modulus KV
180 GPa
Shear Modulus GR
78 GPa
Bulk Modulus KR
180 GPa
Shear Modulus GVRH
82 GPa
Bulk Modulus KVRH
180 GPa
Elastic Anisotropy
0.52
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnCu2Ni (mp-30593) 0.1104 0.005 3
CrCoPt2 (mp-570863) 0.0480 0.000 3
LiCa6Ge (mp-12609) 0.0023 0.180 3
GaFeNi2 (mp-1065359) 0.0399 0.066 3
GaCo2Ni (mp-1018060) 0.0144 0.075 3
Cr8Ni50Mo15W2 (mp-767372) 0.2144 0.028 4
CrFeCoNi (mp-1012640) 0.3598 0.118 4
CrFeCoNi (mp-1096923) 0.4011 0.193 4
PmTm3 (mp-982881) 0.0000 0.031 2
SmHo3 (mp-972607) 0.0006 0.024 2
PrNd3 (mp-975887) 0.0000 0.015 2
Pa3Al (mp-862848) 0.0006 0.000 2
FeNi3 (mp-1007855) 0.0001 0.241 2
Sc (mp-36) 0.0013 0.049 1
Xe (mp-611517) 0.0023 0.006 1
Eu (mp-623532) 0.0023 0.035 1
He (mp-614456) 0.0023 0.008 1
Au (mp-81) 0.0023 0.000 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: V_pv Pd
Final Energy/Atom
-6.3900 eV
Corrected Energy
-25.5601 eV
-25.5601 eV = -25.5601 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 108677
Submitted by
User remarks:
  • Palladium vanadium (3/1) - LT

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)