Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.312 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.002 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.44 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToHgI2 |
Band Gap1.379 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP42/nmc [137] |
HallP 4n 2n 1n |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 167.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 83.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 242.4 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 83.7 |
CdTe (mp-406) | <1 1 0> | <1 0 0> | 121.2 |
TiO2 (mp-2657) | <0 0 1> | <1 1 0> | 171.4 |
TiO2 (mp-2657) | <1 0 0> | <0 0 1> | 83.7 |
Mg (mp-153) | <1 0 1> | <1 1 0> | 171.4 |
InSb (mp-20012) | <1 1 0> | <1 0 0> | 121.2 |
BaTiO3 (mp-5986) | <0 0 1> | <1 0 0> | 242.4 |
YAlO3 (mp-3792) | <0 1 1> | <1 0 1> | 147.3 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 251.1 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 121.2 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 251.1 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 171.4 |
KCl (mp-23193) | <1 1 1> | <1 0 1> | 147.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 167.4 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 83.7 |
TePb (mp-19717) | <1 1 0> | <1 0 0> | 121.2 |
TePb (mp-19717) | <1 1 1> | <1 0 1> | 147.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 251.1 |
LiNbO3 (mp-3731) | <1 1 0> | <0 0 1> | 251.1 |
Al (mp-134) | <1 0 0> | <1 0 0> | 242.4 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 1> | 190.8 |
CdTe (mp-406) | <1 1 1> | <1 0 1> | 147.3 |
LiTaO3 (mp-3666) | <1 1 0> | <0 0 1> | 251.1 |
TiO2 (mp-2657) | <1 0 1> | <0 0 1> | 251.1 |
C (mp-66) | <1 0 0> | <0 0 1> | 167.4 |
InSb (mp-20012) | <1 1 1> | <1 0 1> | 147.3 |
NaCl (mp-22862) | <1 0 0> | <0 0 1> | 167.4 |
YAlO3 (mp-3792) | <1 0 1> | <1 0 1> | 147.3 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <0 0 1> | 167.4 |
SiC (mp-8062) | <1 0 0> | <1 1 0> | 171.4 |
SiC (mp-8062) | <1 1 0> | <1 0 0> | 242.4 |
MgF2 (mp-1249) | <1 1 1> | <1 0 0> | 121.2 |
Ge (mp-32) | <1 0 0> | <0 0 1> | 167.4 |
LiAlO2 (mp-3427) | <1 1 0> | <1 1 1> | 190.8 |
Fe2O3 (mp-24972) | <1 1 0> | <0 0 1> | 251.1 |
Fe2O3 (mp-24972) | <1 1 1> | <0 0 1> | 251.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
5.12 | 0.00 | 0.00 |
0.00 | 5.12 | 0.00 |
0.00 | 0.00 | 4.56 |
Dielectric Tensor εij (total) |
||
---|---|---|
10.44 | 0.00 | 0.00 |
0.00 | 10.44 | 0.00 |
0.00 | 0.00 | 6.18 |
Polycrystalline dielectric constant
εpoly∞
4.93
|
Polycrystalline dielectric constant
εpoly
9.02
|
Refractive Index n2.22 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
InPS4 (mp-20790) | 0.6231 | 0.000 | 3 |
K2B2S7 (mp-4351) | 0.5548 | 0.000 | 3 |
GaCuI4 (mp-29403) | 0.4728 | 0.000 | 3 |
AlCuCl4 (mp-28020) | 0.5177 | 0.000 | 3 |
GaCuCl4 (mp-29362) | 0.4737 | 0.000 | 3 |
HgI2 (mp-567471) | 0.0659 | 0.005 | 2 |
HgI2 (mp-583213) | 0.1343 | 0.000 | 2 |
NiS2 (mvc-7056) | 0.2990 | 0.380 | 2 |
HgI2 (mp-23192) | 0.2791 | 0.001 | 2 |
WS2 (mvc-7053) | 0.2187 | 0.753 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Hg I |
Final Energy/Atom-1.4292 eV |
Corrected Energy-34.2998 eV
-34.2998 eV = -34.2998 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)